Precision Machined Grade 2 Titanium Stepped Shafts
video
Precision Machined Grade 2 Titanium Stepped Shafts

Precision Machined Grade 2 Titanium Stepped Shafts

Precision Machined Grade 2 Titanium Stepped Shafts
Material:CP Grade 2,Grade 3;Titanium alloy Grade 5,Grade 7,Grade 12,etc
Type:Machined & Drilled, Polished
Size:Can produce according to customer design or drawing/sketches
MOQ: 10pcs
Send Inquiry
Description

Products introduction

 

The Precision Machined Grade 2 Titanium Stepped Shafts are a multi-diameter stepped shaft component manufactured from ASTM B348 / ASME SB348 Gr2 industrial-grade pure titanium bar through precision machining processes such as CNC turning, milling, and grinding.

It is classified as a machined pure titanium component, not a titanium alloy (Gr5 is the Ti-6Al-4V alloy). Within the titanium grade series, GR2 is an industrial-grade pure titanium characterized by low strength, high ductility, excellent corrosion resistance, and ease of machining; it is the most widely used titanium grade in the chemical, marine, and medical device industries.

The core feature of a stepped shaft is multiple cylindrical sections of varying diameters distributed along a single shaft, which are used to mount bearings, seals, gears, couplings, or valve cores to achieve axial positioning and torque/fluid transmission.

 

GR2 Material Chemical Composition

 

Elements Ti Fe C N H O Other Single Other Totals
GR2 Balance ≤0.30 ≤0.08 ≤0.03 ≤0.015 ≤0.25 ≤0.10 ≤0.40

 

Mechanical Properties at Room Temperature

 

Performance Typical values Explanation
Tensile Strength (UTS) ≥345 MPa(50 ksi) ASTM Minimum Value
Yield Strength YS ≥275 MPa(40 ksi) 0.2% Residual deformation
Elongation El ≥20% Gauge Length 4D
Cross-sectional Contraction Ratio RA ≥30% -
Modulus of Elasticity E ~105 GPa About 1/2 that of steel
Density ρ 4.51 g/cm³ About 57% that of steel
Hardness HB ~120~200 In response to fluctuations in oxygen content
Thermal Conductivity 16 W/(m·K) Only 1/4 the weight of stainless steel
Coefficient of Linear Expansion 8.6×10⁻⁶ /℃ Similar to borosilicate glass; suitable for titanium-glass sealing

 

Product Design Features

 

A stepped shaft consists of multiple shoulders, journal sections, and transition sections. Common features include cylindrical surfaces, shoulder end faces, center holes, keyways, threads, relief grooves, chamfers, and fillets.
Precision components are typically controlled according to the following specifications:

  1. Dimensional tolerances: Shaft necks are typically controlled to IT6–IT7, with high-precision parts reaching IT5; specific requirements depend on the nature of the fit.
  2. Roundness/Cylindricity: Precision shafts are often within the micrometer range, depending on diameter and manufacturing capabilities.
  3. Coaxiality/Radial Runout: Critical shaft necks typically require tolerances in the 0.01–0.03 mm range, with even stricter requirements for high-speed rotating shafts.
  4. Surface roughness: Shaft necks are typically Ra 0.2–0.8 μm; sealing surfaces in mating fits may require finer finishes
  5. Straightness: Particularly important for long shafts, as it is significantly affected by heat, cutting forces, and clamping
  6. Perpendicularity of shaft shoulders, end face runout, keyway symmetry, thread accuracy, etc.
  7. Surface integrity: Avoid grinding burns, microcracks, folding, visible tool marks, and excessively deep work-hardened layers
  8. Non-destructive testing: PT (dye penetrant/fluorescent penetrant) and UT (ultrasonic testing) may be performed as needed; critical load-bearing shafts may also require etching inspection or low-magnification microstructural examination

 

Key Technical Specifications

 

 

  • Diameter: 20–600 mm (typically Φ40–300 mm)
  • Length :100–6000 mm (typically ≤3000 mm)
  • Weight per piece: 5–2000+ kg
  • Coaxiality: ≤0.1 mm/m (typical value)
  • Surface Roughness: Ra 0.8–3.2 μm
  • Dimensional Tolerances: As per customer drawings or technical agreements
  • Delivery Condition: Annealed

 

Corrosion Resistance

 

GR2 performs significantly better than 304/316L stainless steel in the following media:

- Seawater: Virtually no corrosion in either fully submerged or splash zones, with an annual corrosion rate of < 0.0025 mm/year; it is the material of choice for marine engineering
- Chloride solutions: No pitting or stress corrosion cracking (SCC) in NaCl, MgCl₂, and CaCl₂-a critical weakness of 316L and duplex stainless steels
- Oxidizing acids: Wet chlorine gas, sodium hypochlorite, nitric acid (<50% concentration, room temperature to boiling point)
- Alkaline solutions: NaOH, KOH-corrosion resistance superior to that of stainless steel
- Alternating wet and dry atmospheres: Especially in coastal and chemical atmospheres, the surface remains lustrous after ten years
- Food/pharmaceutical grade: No ion leaching; compliant with FDA and USP Class VI

 

Products showcase

Precision Machined Grade 2 Titanium Stepped Shafts

 

Precision Machined Grade 2 Titanium Stepped Shafts
Precision Machined Grade 2 Titanium Stepped Shafts factory
Precision Machined Grade 2 Titanium Stepped Shafts supplier
Precision Machined Grade 2 Titanium Stepped Shafts manufacturer
Precision Machined Grade 2 Titanium Stepped Shafts wholeseller
Precision Machined Grade 2 Titanium Stepped Shafts in stocks

Applications

 

1 Chemical / Petrochemical (Largest Segment)

- Valve stems, valve plugs, and valve seats: Internal components of control valves, globe valves, and butterfly valves, exposed to hydrochloric acid tail gas, chlorine, and brine
- Pump shafts: Main shafts for titanium pumps (chemical process pumps, seawater pumps)
- Centrifuge main shafts: Corrosion-resistant centrifuges, scraper centrifuges
- Heat exchanger tube sheets and spacer tubes

2 Offshore Engineering / Marine

- Seawater desalination units: High-pressure pump shafts and impellers
- Subsea Christmas tree stem
- Ship ballast water systems and fire pump shafts
- Offshore wind power: Corrosion-resistant fasteners for tower interiors and hydraulic valve stems

3 Medical / Pharmaceutical

- Surgical instrument drive shafts: orthopedic drills, milling cutter shafts
- Pharmaceutical equipment: centrifuge shafts, mixer shafts (must meet FDA and GMP requirements for no leaching)
- Implant components: orthopedic instruments, surgical tools (Note: The implanted bone itself uses Ti-6Al-4V ELI / Gr23, not GR2)

4 Vacuum / Semiconductor / High-Purity Fluids

- Vacuum equipment drive shafts: Non-magnetic titanium with low outgassing rate
- High-purity chemical transfer: Metal skeleton shafts for PFA/PVDF-lined valves
- LCD / photovoltaic equipment: Corrosion-resistant conveyor roller shafts

5 Food / Pharmaceutical / Environmental Protection

- Agitator shafts and pump shafts in production equipment for monosodium glutamate, citric acid, and lactic acid
- Pump shafts and agitator shafts in hydrometallurgy (copper, nickel, and cobalt extraction)
6 Aerospace (Secondary)

- GR2 has lower strength than Gr5; Gr5 is used for primary load-bearing components in aerospace applications; GR2 is primarily used in piping systems, non-load-bearing structural components, and fasteners

 

Summary of Product Advantages

 

Outstanding corrosion resistance: Resists corrosion during long-term use in seawater, chloride solutions, and various acidic and alkaline media; its service life far exceeds that of stainless steel shaft products.

High specific strength: With a density of only 60% that of steel, it significantly reduces weight under equivalent load-bearing conditions.

Non-magnetic and excellent weldability: Suitable for special applications where magnetic properties are a concern or where welded assembly is required.

Medium Strength and High Ductility: Balances structural load-bearing capacity with machinability and formability; features a low yield-to-tensile strength ratio, ensuring excellent safety in use.

Fully Controlled Precision Throughout the Entire Process: From forging billets to precision grinding, multiple stress-relief heat treatment processes combined with scientific allocation of machining allowances consistently achieve high precision levels with radial dimensional tolerance ≤±0.015 mm, concentricity ≤0.02 mm, and surface roughness Ra ≤0.8 μm.

 

about our factory

who we are?

One-stop Titanium Processing Parts Factory in China

 

We Baoji Reliab Metal Material Co.,Ltd was founded in year 2014, located in the famous 'China Titanium Valley--BAOJI', under the strong R&D ability and continuously development, our mainly products have including titanium&titanium alloy bars/rods, plates, tubes, forgings, fasteners&machined parts, also zirconium and nickel products.

We have passed the Quality System Certificate of ISO 9001-2015, aiming for the satisfactions of different customers' requests.

Precision Machined Grade 2 Titanium Stepped Shafts

contact us

 

Precision Machined Grade 2 Titanium Stepped Shafts E-mail: garychen3215@hotmail.com

Precision Machined Grade 2 Titanium Stepped Shafts Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

Precision Machined Grade 2 Titanium Stepped Shafts Contact: Mr. Gary Chen

Precision Machined Grade 2 Titanium Stepped Shafts Phone: +86-917-8883215

Precision Machined Grade 2 Titanium Stepped Shafts Mobile/WhatsApp: +86 13092900605

Hot Tags: precision machined grade 2 titanium stepped shafts, China precision machined grade 2 titanium stepped shafts manufacturers, suppliers, factory, m3 titanium bolts, silver titanium, titanium bolts for sale, titanium cap screws, titanium thumb screw, titanium welder parts

Send Inquiry

(0/10)

clearall