Home > News > Content

Methods For Testing The Hardness Of Titanium And Titanium Alloys

Oct 07, 2026

There are many methods for testing the hardness of titanium materials, and different methods are suitable for different material types, hardness ranges, and testing scenarios. The following is an overview of each method.

I. Standard Laboratory Methods Using Indentation (Preferred for Arbitration)

1. Vickers Hardness HV (Most Recommended in the Titanium Industry; Preferred for Welds and Microstructure)

Standard: ASTM E384
Principle: A 136° diamond quadrangular pyramid indenter is used to apply a load; the HV value is calculated based on the diagonal of the indentation.

- Macro Vickers (HV5, HV10): Hardness of forgings, bars, and sheet metal matrices;
- Micro Vickers (HV0.05–HV1): Hardness of welds, heat-affected zones, nitrided/anodized surface layers, small specimens, and metallographic grain/phase regions.
Advantages: Wide load range, small indentation, low elastic modulus of titanium, minimal indentation rebound, and stable readings; suitable for nearly all titanium materials, including Gr5, and pure titanium Gr2; widely recognized in international trade reports.
Disadvantages: Specimens require polishing; testing is slow.

2. Rockwell Hardness HR (Rapid Batch Testing on Production Lines)

Standard: ASTM E18
Indentation depth method, multiple scales; commonly used for titanium:

- HRB: Annealed pure titanium, soft titanium alloys (Gr1/Gr2);
- HRC: Age-hardened titanium alloys (age-hardened Gr5,and other high-strength forgings);
- Surface Rockwell HR15N/HR30N: Thin sheets, thin-walled titanium tubes, and surface-hardened thin layers.
Advantages: Fast testing, simple sample preparation, small indentation size; suitable for batch quality inspection of incoming materials; widely used in factory acceptance testing of titanium bars and forgings for export.
Disadvantages: Not suitable for thin sections, curved surfaces, or weld zones; surface scale can cause a 2–4 HRC error and must be ground off.

3. Brinell Hardness HBW (cast titanium, coarse-grained, large cross-sections)

Standard: ASTM E10
Cemented carbide ball indenter (ordinary steel balls are prohibited, as titanium can deform the steel ball and cause errors); F/D² is set to 30.
Applications: Cast titanium alloy Gr5, large forgings; produces a large indentation that reflects the average hardness of the region and provides good representativeness for samples with non-uniform microstructure.
Disadvantages: Large indentation; destructive test; cannot be used on thin sheets or precision-machined finished parts.

4. Knoop Hardness HK (Ultra-thin titanium foil, extremely thin surface layers)

Standard: ASTM E384
Diamond indenter with a rhombic shape, producing a long indentation. Suitable for extremely thin titanium strips, coated surfaces, and shallow diffusion layers; the indentation is very shallow, making it more suitable for thin layers than the micro-Vickers test; commonly used for anodized titanium surfaces.

Special Precautions for Titanium Testing

1. Titanium has a low modulus of elasticity, and its indentation rebound effect is greater than that of steel; therefore, scale and turning marks must be removed from the specimen surface;
2. For Brinell testing, a carbide ball must be used for HBW; steel balls for HBS cannot be used on titanium alloys;
3. For thin-walled tubes, the Vickers or surface Rockwell methods are preferred to avoid penetration;

ASTM B381 Titanium forging ringsTitanium hardness testing machine

High Precision TI6AL4V Titanium Alloy Tubes E-mail: garychen3215@hotmail.com

High Precision TI6AL4V Titanium Alloy Tubes Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

High Precision TI6AL4V Titanium Alloy Tubes Contact: Mr. Gary Chen

High Precision TI6AL4V Titanium Alloy Tubes Phone: +86-917-8883215

High Precision TI6AL4V Titanium Alloy Tubes Mobile/WhatsApp: +86 13092900605

 

Send Inquiry
Contact Us
    • Baoji Reliab Metal Materials Co.,Ltd
    • Mobile:+8613092900605
                     +8613092913521
    • E-mail:garychen3215@hotmail.com
                     boantj@163.com
    • Web:www.reliabmetal.com
    • Address:No.35 Middle of Baoti Road, Hi-Tech Development Zone, Baoji city, Shaanxi province China 721000