Titanium Tube

Your Professional Titanium Tube Supplier!

 

 

Baoji Reliab Metal Materials Co.,Ltd has focused on top-quality titanium/nickel mill products and titanium alloy machined parts for over 12 years in China. We are one of the leading suppliers in China's titanium and nickel products industry. Our main products include: titanium/nickel bars, plates, tubes, forgings, fasteners, and CNC machined parts.

 

 
  • Seamless Durable And Corrossion-Resistant Titanium Tubes
    Seamless Durable And Corrossion-Resistant Titanium Tubes

    Seamless Durable and Corrossion-Resistant Titanium TubesMaterial Grade:Gr2,Gr3,Gr5,Gr9,Ti-0.3Mo-0.8Ni,Ti-0.2Pd,etcStandard:ASTM B337,B338,B861Size:OD5.0mm-219mm*Thk0.1mm-10mmLength:Normally less than
    Add to Inquiry
  • Extruded Titanium Tubing
    Extruded Titanium Tubing

    Extruded titanium tubingMaterial:Gr1,Gr2,Gr3,Gr5,Gr5ELI,Ti-0.3Mo-0.8Ni,Ti-3Al-2.5VSize:φ25mm-φ700mm*WT1mm-10mm*LengthFeatures:High strength,corrosion-resistant,lightweightOur unique feature:Custom
    Add to Inquiry
  • Titanium Welded Tube ASTM B337
    Titanium Welded Tube ASTM B337

    Titanium welded tubes are tubular products manufactured by rolling titanium and titanium alloy sheets or strips into a tube shape and welding them along the longitudinal axis. Compared to seamless
    Add to Inquiry
  • Titanium U Bend Pipe Grade 2
    Titanium U Bend Pipe Grade 2

    Titanium U Bend Pipe Grade 2Material:Titanium Grade 1,Grade 2Shape:U-Shape,L-Shape,etcFinish:Sandblasting;Polished;Acid washingFeatures:Can be customized according to design/drawingMOQ:10pcs
    Add to Inquiry
  • Bending Titanium Pipes For Aerospace Engineering
    Bending Titanium Pipes For Aerospace Engineering

    Bending titanium pipes for aerospace engineeringMaterial:Titanium Grade 2,Grade 5(Ti-6Al-4V),Gr7,Gr23(TI-6AL-4V ELI)Finish:Polished;Sandblasted;Acid washed.Size:Custom size and specsMethods:Cold
    Add to Inquiry
  • Aerospace Ti-6Al-4V Seamless Titanium Tubing
    Aerospace Ti-6Al-4V Seamless Titanium Tubing

    Aerospace Ti-6Al-4V Seamless Titanium TubingMaterial:Titanium alloy Grade 5(Ti-6Al-4V)Outside Diameter:Dia5mm-200mmWall thickness:0.5mm-20mmLength:500mm-6000mm, can cut into any
    Add to Inquiry
  • Gr5 Titanium Seamless Pipes
    Gr5 Titanium Seamless Pipes

    Gr5 Titanium seamless pipesMaterial:Titanium Grade 5(Ti-6Al-4V)Standard:ASTM B337,ASTM B338,ASTM B861Size:OD10mm-200mm*Length MOQ:1 pieceFeature:Custom size and specs.
    Add to Inquiry
  • Titanium Tubing For Bicycle
    Titanium Tubing For Bicycle

    1.Titanium tubing for bicycle2.Materials:CP Titanium Gr2,Titanium alloy Gr5(TI-6AL-4V),Titanium alloy Gr9(Ti-3AL-2.5V)3.Standard:ASTM B338,ASTM B861,AMS
    Add to Inquiry
  • Grade 2 Titanium Tube Bending
    Grade 2 Titanium Tube Bending

    1.Grade 2 titanium tube bending2.Material:Titanium Grade 1,Grade 2,Grade 3,Grade 9,Grade 123.Standard:ASTM B338,AMS 49424.Surface:Free of cracks,wrinkles,scratches,and scale;bright after acid
    Add to Inquiry
  • Titanium Rectangular Tube
    Titanium Rectangular Tube

    1.Item name:Titanium rectangular tube2.Material:Gr1,Gr2,Gr5,Gr7,Gr93.Standard:ASTM B338,ASTM B861,JIS H46004.Types:Seamless titanium rectangular tube,welded titanium rectangular tube,Cold-formed
    Add to Inquiry
  • Hollow Titanium Rods
    Hollow Titanium Rods

    Hollow titanium rods1.Material:Gr1,Gr2,Gr5 (Ti-6Al-4V),Gr9 (Ti-3Al-2.5V),Gr7/Gr122.Outside diameter:3mm-426mm(Full coverage of capillaries and medium to large diameter)3.Standard:ASTM B337,ASTM
    Add to Inquiry
  • 6Al4V Titanium Tubing
    6Al4V Titanium Tubing

    Item name:6Al4V Titanium tubingMaterial:CP titanium Gr1,Gr2,Titanium alloy Gr5,Gr7,Gr9,Gr12Standard:ASTM B337,ASTM B338,ASTM B861Size:OD range 3mm-219mm,WT range0.5mm-10mmLength:Less than 6000mmOur
    Add to Inquiry
First 123 Last 1/3
 
Why Choose Us

Professional Team

The company has more than 110 production workers and more than 35 R&D personnel, forming an experienced and technically solid professional team.

Quality Control

Our products meet international standards such as ASTM F67 and ASTM F136 to ensure stable and reliable product quality.

Advanced Equipment

We are equipped with a series of advanced production equipment, including VAR vacuum melting furnace, 4500T hydraulic press, 800T fast forging press, vacuum annealing furnace, grinder, vertical lathe, three-axis machining center and five-axis machining center.

Sales Market

Our products are exported to many countries and regions such as the United States, the United Kingdom, Germany, France, Japan, Italy, Russia, South Korea, Thailand, the Philippines, Singapore, Poland, Australia, India, New Zealand and Mexico.

 

 

Titanium Tube Specification

 

 

Tube Type

Dimensions,mm

Grade

Standard

Seamless Tube

Dia3~114mm*Tk0.2~6.0mm*L

Gr1, Gr2, Gr7,Gr9, Gr11,Gr12

ASTM B337, ASTM B338

Extruded Tube

Dia25~210mm*Tk6.0~30.0mm*L

Q/BS5631

Square Tube

Dia25~210mm*Tk6.0~30.0mm*L

ASTM B337, ASTM B338

Welded Tube

Dia25~210mm*Tk6.0~30.0mm*L

ASTM B862

 

 

Advantages Of Titanium Tube

 

 

 

Low density
Titanium tube incorporates a low weight to high strength ratio. The density of titanium is less than stainless steel, nickel and copper, which makes it easier to work with.

 

Durability
Our products can be tailored to suit your specific requirements. As a transition metal, titanium tube is renowned for its high strength.

 
 

Corrosion resistance
The titanium tubes are renowned for their ability to resist corrosion and other impacts. Our titanium tubes are manufactured to suit highly corrosive environments, allowing you to maintain a high-quality appearance.

 
 

Chemical resistance
Titanium tubes are not only able to resist corrosion; they're designed to withstand chemical components too. We supply the titanium tubes in an assortment of grades, ranging from Grade 1 to 12.

 
 

Heat transfer
Our titanium tube supplies work well under extreme temperatures and pressures so you needn't worry about getting the most out of your equipment.

 
 

High performance
The titanium tubes are considered to be some of the most versatile of their calibre. Titanium is a metal that combines high strength with low density to perform exceptionally well under pressure.

 

 

 

Titanium Tube Mechanical Properties

 

 

Hardness, Rockwell B

98

98

Shear Modulus

38 MPa

5510 ksi

Shear Strength

380 MPa

55100 psi

Tensile Strength, Ultimate

430 MPa

62400 psi

Tensile Strength, Yield

340 MPa

49300 psi

Elongation at Break

28%

28%

Charpy Impact

65 J

47.9 ft-lb

V-notch

 

 

Titanium Pipe Grades

 

 

Grade

N(≤)

C(≤)

H(≤)

Fe(≤)

O(≤)

Al(≤)

V(≤)

Pd(≤)

Mo(≤)

Ni(≤)

Ti

GR1

0.03

0.08

0.015

0.2

0.18

/

/

/

/

/

Bal

GR2

0.03

0.08

0.015

0.3

0.25

/

/

/

/

/

Bal

GR3

0.05

0.08

0.015

0.3

0.35

/

/

/

/

/

Bal

GR4

0.05

0.08

0.015

0.2

0.4

/

/

/

/

/

Bal

GR5

0.05

0.08

0.015

0.4

0.2

5.5~6.75

3.5~4.5

/

/

/

Bal

GR7

0.03

0.08

0.015

0.3

0.25

/

/

0.12~0.25

/

/

Bal

GR9

0.03

0.08

0.015

0.25

0.15

2.5~3.5

2.0~3.0

/

/

/

Bal

GR12

0.03

0.08

0.015

0.3

0.25

/

/

/

0.2~0.4

0.6~0.9

Bal

GR23

0.05

0.08

0.012

0.25

0.13

5.5~6.5

3.5~4.5

 

 

 

Bal

 

 
Titanium Tube Applications
 
01/

Aerospace
Used in aircraft structures, engine components, and hydraulic systems due to their high strength-to-weight ratio and resistance to corrosion.

02/

Medical
Employed in medical implants such as bone plates, dental implants, and surgical instruments due to their biocompatibility and corrosion resistance.

03/

Chemical Processing
Utilized in chemical reactors, heat exchangers, and piping systems due to their resistance to corrosion by acids and chemicals.

04/

Power Generation
Found in power plants for heat exchangers, condensers, and steam turbine components due to their high-temperature strength and corrosion resistance.

05/

Oil and Gas Industry
Used in offshore drilling rigs, subsea pipelines, and refinery equipment due to their resistance to corrosion in harsh environments.

06/

Automotive
Employed in exhaust systems, hydraulic lines, and suspension components for their lightweight nature and resistance to high temperatures and corrosion.

07/

Sports and Recreation
Utilized in bicycle frames, golf club shafts, and marine equipment due to their lightweight and durable properties.

08/

Architectural Design
Found in architectural structures such as handrails, support beams, and artistic installations for their aesthetic appeal and durability..

 

 

Stock Range

We have the stocks for most of the normal sizes/specs for different grades of titanium and titanium alloy, and can make to order for special sizes.

  • Stock grades: Gr1,Gr2,Gr3,Gr5, Gr7,Gr9,Gr12
  • Standard: ASTM B337,ASTM B338,ASTM B861,ASTM B862
  • Surface: Polished,Acid,Blasted
  • Outside diameter: OD8mm~219mm
  • Wall thickness:0.5mm~20mm
  • Length:10mm~6000mm
  • Applications: Chemical industry, Sports bicycle parts, Marine engineering, etc.
Gr2 Seamless Titanium Tube

 

 

Packaging and Shipping

 

 

Packaging

Be packed with Standard export plywood case.

Transportation methods

By standard express(such as UPS, DHL, Fedex, TNT); BY Air Cargo; By sea/ocean.

 

 

Trade Terms

 

 

Payment methods

T/T, L/C, Credit Card, Paypal, Western Union

Trade terms

FOB, CIF, C&F, DDP

Delivery time

3~15 days

 

 

FAQ

 

 

Q: What is a titanium tube used for?

A: Titanium tube has lightweight, high strength, and superior mechanical properties. It is widely used in heat exchange equipment, such as tube heat exchangers, coil tube heat exchangers, serpentine tube heat exchangers, condensers, evaporators, and conveying pipes.

Q: How hard is it to bend titanium tubing?

A: Without a specialized titanium tube bending machine, it's almost impossible. Even with manual tube benders, the process can take a lot of effort to bend/form even a thin titanium tube. Even hot bending requires a certain degree of effort and lots of time.

Q: How strong is titanium tubing?

A: The softest grade of commercially pure titanium is around 240 MPa, while high-strength alloys can go as high as 1,400 MPa. Biocompatible and nontoxic, titanium tubing is often used in more challenging, complex applications, such as surgical instruments and orthopedic implants.

We're professional titanium tube manufacturers and suppliers in China, featured by quality products and good price. Please rest assured to buy titanium tube for sale here from our factory. For customized service, contact us now.

nano titanium dioxide, 3 inch titanium tubing, 2 titanium tubing

(0/10)

clearall