Baoji Reliab Metal Materials Co.,Ltd has focused on top-quality titanium/nickel mill products and titanium alloy machined parts for over 12 years in China. We are one of the leading suppliers in China's titanium and nickel products industry. Our main products include: titanium/nickel bars, plates, tubes, forgings, fasteners, and CNC machined parts.
-
Grade 9 Titanium Alloy Forged Round RingGrade 9 Titanium alloy forged round ringStandard:ASTM B381,AMS 4928Size:OD100-500mm,ID 80-450mm,H10-500mmFinish:AnnealedAdd to Inquiry
-
High Performance Titanium Alloy Forging RingsHigh performance titanium alloy forging ringsMaterial:CP Titanium Grade 1,Grade 2,Grade 3;Titanium alloy Grade 5,Grade 7,Grade 9,Grade 12Standard:ASTM B381,AMS 4928,ISOAdd to Inquiry
-
Dental Titanium Cutting DiscProduct name:Dental Titanium Cutting DiscMaterial:Titanium Gr23(TI6AL4V ELI),Grade 3,Grade 4Shape:Round,SquareSize:Dia98mm*10mm/12mm/14mm/16mm/18mm/20mm/25mmMOQ: 10pcsOur feature:Custom size and specsAdd to Inquiry
-
Gr7 Titanium Forged RingGr7 titanium alloy (Ti-0.2Pd), a palladium-enhanced industrial pure titanium, has become a core material for equipment in extreme environments with its ultra-low corrosion rate of 0.001mm/a andAdd to Inquiry
-
Titanium Grade 2 ForgingsTitanium alloy forging rings and forgings are widely used in high-tech fields such as aviation, aerospace, medical treatment, and chemical industry. They have become the ideal choice in the industryAdd to Inquiry
-
High Quality Titanium Grade 2 Forged RingItem name: High quality titanium grade 2 forged ringMateril: CP titanium grade 2, grade 3Standard: ASTM B381Producing type: Forged,MachinedAdd to Inquiry
-
High Performance Titanium Target For PVDItem name:High performance titanium target for PVDPurity:99.5%,99.8%,99.9%Shape:Round shapeDiameter:OD95/95/100/152.4mmMOQ: 1 piceceAdd to Inquiry
-
High Purity Titanium Sputtering TargetsItem name:High purity titanium sputtering targetsMaterial:Pure titanium Grade1, Grade 2Shape:Round target, Square targetPurity:99.9% 3N, 4N, 4N5Finish:CNC MachinedAdd to Inquiry
-
Gr5 Titanium Aerospace ForgingsItem name:Gr5 titanium aerospace forgingsMaterial:Ti-6AL-4V,Grade 5, Grade 5 ELIProcessing:Forging,MachiningStandard:ASTM B381, AMS4928Add to Inquiry
-
TI6AL4V Titanium Alloy Forged BilletsItem name:TI6AL4V titanium alloy forged billetsBrand:RELIABMaterial:TI-6AL-4V, Grade 5 Titanium alloySize:Dia50~350mmLength: 50~3000mmAdd to Inquiry
-
Gr5 Titanium Alloy Square BlocksItem name:Gr5 Titanium alloy Square BlocksMaterial:Gr1, Gr2, Gr3, Gr4, Gr5, Gr7, Gr9, Gr23Standard: ASTM B381 , ASTM F67, ASTM F136, AMS 4928Shape: Square, Rectangular block, Round disc, RoundAdd to Inquiry
-
Dental Titanium Disc Grade 5Item name: Dental Titanium Disc Grade 5Material: Gr1, Gr2, Gr3, Gr4, Gr5, Gr23, Ti6Al7NbStandard: ASTM F67, ASTM F136, ISO 5832-2, ISO 5832-3Shape: Round, SquareMOQ: 1 PieceTitanium discs forAdd to Inquiry
- Baoji Reliab Metal Materials Co.,Ltd
- Mobile:+8613092900605
+8613092913521 - E-mail:garychen3215@hotmail.com
boantj@163.com - Web:www.reliabmetal.com
- Address:No.35 Middle of Baoti Road, Hi-Tech Development Zone, Baoji city, Shaanxi province China 721000
Why Choose Us
Professional Team
The company has more than 110 production workers and more than 35 R&D personnel, forming an experienced and technically solid professional team.
Quality Control
Our products meet international standards such as ASTM F67 and ASTM F136 to ensure stable and reliable product quality.
Advanced Equipment
We are equipped with a series of advanced production equipment, including VAR vacuum melting furnace, 4500T hydraulic press, 800T fast forging press, vacuum annealing furnace, grinder, vertical lathe, three-axis machining center and five-axis machining center.
Sales Market
Our products are exported to many countries and regions such as the United States, the United Kingdom, Germany, France, Japan, Italy, Russia, South Korea, Thailand, the Philippines, Singapore, Poland, Australia, India, New Zealand and Mexico.
Titanium Forgings Specification
|
Al |
V |
C Max |
Fe Max |
H Max |
N Max |
O Max |
Ti,min |
|
5.5~6.75 |
3.5~4.5 |
0.08 |
0.40 |
0.015 |
0.05 |
0.20 |
90 |
Advantages of Titanium Forgings
Enhanced Mechanical Properties
One of the primary advantages of titanium forgings is the enhancement of mechanical properties. The forging process aligns the metal's grain structure, resulting in improved strength and toughness.
Weight Reduction
In industries where weight is a critical factor, such as aerospace and automotive, titanium forgings offers significant weight reduction without compromising strength.


Corrosion Resistance
Titanium's exceptional corrosion resistance is a significant advantage in many applications. Forged titanium components can withstand harsh environments, reducing the need for protective coatings and maintenance.
Design Flexibility
Titanium forgings allows for greater design flexibility compared to other manufacturing processes. The ability to create complex shapes and geometries enables engineers to optimize designs for performance and functionality.
Mechanical Property of Titanium Forgings
|
Grade |
Tensile Strength,min |
Yield Strength,min |
Elongation,% |
||
|
Ksi |
MPa |
Ksi |
MPa |
||
|
Gr 1 |
35 |
240 |
20 |
138 |
24 |
|
Gr 2 |
50 |
345 |
40 |
275 |
20 |
|
Gr 3 |
65 |
450 |
55 |
380 |
18 |
|
Gr 4 |
80 |
550 |
70 |
483 |
15 |
|
Gr 5 |
130 |
895 |
120 |
828 |
10 |
|
Gr7 |
50 |
345 |
40 |
275 |
20 |
|
Gr 9 |
90 |
620 |
70 |
483 |
15 |
|
Gr 12 |
70 |
483 |
50 |
345 |
18 |
|
Gr 23 |
120 |
828 |
110 |
759 |
10 |
Titanium Forging Process
● The titanium billets are always heated to a certain temperature, usually between 1,600°F and 2000°F. It is from this controlled heating that the fabric gets softened to be malleable for shaping while ensuring that its chemical composition and structural integrity remain intact.
● Once heated, the titanium is conventionally used for great firmness press machines or hammering tool that is capable of giving many tons of pressure. High compressive forces applied from these machines press and squeeze the titanium into whatever shape required, be it a smooth geometric element or a detailed problem.
● Once the titanium is stable into form, it undergoes a cooling technique below cautiously managed situations. Depending on the favored residences of the very last product, this can contain speedy cooling, collectively with quenching in water or oil, to acquire particular hardness degrees.
● The solid titanium issue is then subjected to a sequence of put up-forging techniques to refine it for its final software program. This can include machining to gain specific dimensions, warmness remedies to further regulate its mechanical houses, or surface completing strategies in conjunction with polishing or coating to decorate its look and resistance to put on or corrosion.
Titanium Forgings Applications
Medical
Titanium forgings are ideal for producing biocompatible implants, surgical instruments, and prosthetics, offering durability and compatibility with the human body.
Marine
Forged titanium components are used in shipbuilding, offshore structures, and marine equipment, thanks to their excellent corrosion resistance in seawater.
Automotive
Applied in high-performance vehicle parts like engine components, suspension systems, and exhausts, where strength and weight reduction are critical.
Industrial Applications
Titanium forgings are used in chemical processing, power generation, and oil & gas equipment, where corrosion resistance and durability in harsh environments are essential.
We have the stocks for most of the normal sizes/specs for different grades of titanium and titanium alloy, and can make to order for special sizes.
- Material:CP Gr 2,Gr3; Tialloy Ti-6AL-4VGrade 5, Gr7,Gr9,Gr12
- Processing: Forged, Machined
- Standard: ASTM B381, AMS4928
- Shape: Round Disc, Square disk, Round Rings, Billets, Blocks
- Sizes: Exact size can be customized.
Our Advantages:
- Material Traceability
- Fast Delivery
- Reasonable Pricing
- Quality Guaranteed
- After-Sales Service Guaranteed

Packaging and Shipping
|
Packaging |
Be packed with Standard export plywood case. |
|
Transportation methods |
By standard express(such as UPS, DHL, Fedex, TNT); BY Air Cargo; By sea/ocean. |
Trade Terms
|
Payment methods |
T/T, L/C, Credit Card, Paypal, Western Union |
|
Trade terms |
FOB, CIF, C&F, DDP |
|
Delivery time |
3~15 days |
FAQ
We're professional titanium forgings manufacturers and suppliers in China, featured by quality products and good price. Please rest assured to buy titanium forgings for sale here from our factory. For customized service, contact us now.
titanium forgings, titanium forged billets, tio2 anatase