Nickel Crucibles& Nickel Machined Parts

Nickel Crucibles and Nickel Machined Parts: Custom-Made to Customer Specifications.

 

 

 
  • Slotted Nickel Threaded Rod Studs
    Slotted Nickel Threaded Rod Studs

    Slotted Nickel Threaded Rod StudsMaterial:Ni200,Ni201Type:Half threading,Full threadingFeature:Single-slot grooveMOQ:5pcs
    Add to Inquiry
  • Pure Nickel Flange Nickel Machined Parts
    Pure Nickel Flange Nickel Machined Parts

    Pure nickel flange nickel machined partsMaterial:Nickel 201,Nickel 200Surface:Pickling,grinding,polishingStandard:ASME B16.5,ASME B16.47MOQ: 1piece,custom size acceptable
    Add to Inquiry
  • Pure Nickel Container For Laboratory Use
    Pure Nickel Container For Laboratory Use

    Item name:Pure Nickel container for Laboratory UseMaterial:Nickel 200,Nickel 201Shape:Prototype, square, rectangular, conical, barrel-shapedProcessing
    Add to Inquiry
  • High Purity Pure Nickel Granules
    High Purity Pure Nickel Granules

    Item name:High purity pure nickel granulesPurity:>99.5%,>99.9%Material:Pure nickel 200, Nickel 201Surface:Machined,PolishedMOQ:5kgs
    Add to Inquiry
  • Pure Nickel 200 201 Component Parts
    Pure Nickel 200 201 Component Parts

    Item name:Pure nickel 200 201 component partsMaterial:Nickel 200,nickel 201Purity:99.5%~99.9%Type:Machined,lathed,milled,drilled,polishedShape:Can be customizedMOQ:5pcs
    Add to Inquiry
  • Pure Nickel Box For Scientific Research
    Pure Nickel Box For Scientific Research

    Item name:Pure nickel box for scientific researchMaterial:Nickel 200, Nickel 201Shape:Square 20×30×10mm, Round Φ30–50mm, Capacity 10–100mL;Type:Bend,Welded,PolishedMOQ:1piece
    Add to Inquiry
  • Nickel Alloy 200 Bolt
    Nickel Alloy 200 Bolt

    Item name:Nickel alloy 200 boltStandard:DIN 931,933,934,7991,976,125Head shape:Hex,Square,Round,Hex flange,Flat,T-head & TriangularSize:M3mm-M30mm,customized acceptable
    Add to Inquiry
  • Nickel 200 Hexagon Bolts
    Nickel 200 Hexagon Bolts

    Item name:Nickel 200 hexagon boltsMaterial:Nickel 200,Nickel 201Bolts type:Hexagon full threadingMOQ:50pcs
    Add to Inquiry
  • Nickel 200 Precision CNC Machining Parts
    Nickel 200 Precision CNC Machining Parts

    Item name:Nickel 200 Precision CNC Machining partsMaterial:Nickel 200(UNS N02200),Nickel 201Type:Machined,MilledMOQ:1piece
    Add to Inquiry
  • Welded Nickel Rectangular Crucible
    Welded Nickel Rectangular Crucible

    Item name:Welded Nickel rectangular CruciblePurity:>99.9%Material:Pure nickel 201,nickel 200Size:Thickness 1.5mm*20*40*100mm,2.0mm*15*30*60mm,2.0mm*20*40*100mm;Other size can be customizedMOQ:1piece
    Add to Inquiry
  • Nickel Combustion Boats
    Nickel Combustion Boats

    Item name:Nickel Combustion BoatsPurity:>99.9%Material:Pure nickel 201,nickel 200Size:L=54mm,W=18mm,H=13.3mm;Other size can be customizedMOQ:1piece
    Add to Inquiry
  • High Purity Nickel Crucible With Lid
    High Purity Nickel Crucible With Lid

    Item name:High purity nickel crucible with lidMaterial:Pure nickel 200,nickel 201Shape:Round open with lid, squareMOQ:1 piece
    Add to Inquiry
 
Why Choose Us

Professional Team

The company has more than 110 production workers and more than 35 R&D personnel, forming an experienced and technically solid professional team.

Quality Control

Our products meet international standards such as ASTM F67 and ASTM F136 to ensure stable and reliable product quality.

Advanced Equipment

We are equipped with a series of advanced production equipment, including VAR vacuum melting furnace, 4500T hydraulic press, 800T fast forging press, vacuum annealing furnace, grinder, vertical lathe, three-axis machining center and five-axis machining center.

Sales Market

Our products are exported to many countries and regions such as the United States, the United Kingdom, Germany, France, Japan, Italy, Russia, South Korea, Thailand, the Philippines, Singapore, Poland, Australia, India, New Zealand and Mexico.

 

 

Specification

 

 

Product name

Nickel Machined Parts

Elongation (≥ %)

≥15%

Resistance (μΩ.m)

No resistance

Density

1.75-1.9 G/cm3

Shore Hardness

40-70hsd

Compressive Strength

65-135 Mpa

Melting Point

1435-1445

 

 

Nickel Crucibles&Nickel Machined Parts Key Features

 

 

 

High-Temperature Resistance: Nickel is renowned for its exceptional heat resistance. These crucibles can endure extremely high temperatures, making them ideal for tasks like melting metals, performing high-temperature reactions, and conducting thermal gravimetric analyses (TGA).

 
 

Chemical Compatibility: Nickel is resistant to many corrosive chemicals, acids, and alkalis, ensuring the crucibles' integrity even when exposed to aggressive substances. This resistance is vital for applications involving reactive materials.

 
 

Robust Construction: The crucibles feature a sturdy and durable construction with a 1.0mm wall thickness, offering excellent mechanical strength and resistance to thermal stress.

 
 

Precise Measurements: These crucibles are available in sizes ranging from 30ml to 50ml, providing options for various sample volumes. The graduated markings on the crucibles allow for accurate sample measurements.

 
 

Versatile Applications: Nickel crucibles find utility in a wide range of laboratory applications, including metal alloy analysis, ashing, gravimetric analysis, and the determination of volatile elements.

 
 

Smooth Interior: The crucibles typically have a smooth interior finish, which aids in the easy removal of solid residues after high-temperature processes.

 
 

Lid Compatibility: Many nickel crucibles are designed to accommodate lids or covers, ensuring better control over reactions and sample containment.

 

 

 

Nickel Crucibles Dimensions

 

 

Capacity

Top Dia.

Bottom Dia.

Height

Thickness

(ml)

(mm)

(mm)

(mm)

(mm)

5

21

21

19

0.94

15

36

32

23

0.94

25

40

47

23

0.94

35

40

47

30

0.94

55

40

47

42

0.94

75

51

44

42

0.94

100

59

53

46

0.94

250

83

72

60

0.94

 

Common Types Nickel Crucibles

 

Standard Nickel Crucibles:

General-purpose crucibles for a wide range of sample fusion applications.

Flat Bottom Crucibles:

Ideal for even heat distribution and stability during fusion.

Welded Nickel Rectangular Crucible price

Dimple Crucibles:

Designed with a concave bottom for specific sample retention and melting processes.

Nickel Crucibles with Lids:

Helps to prevent contamination and minimize sample loss.

 

Nickel Crucibles Melting Point

One of the most impressive features of nickel crucibles is their high melting point. Nickel has a melting point of approximately 1455°C (2651°F), making it an excellent choice for a wide range of high-temperature applications. However, it's important to note that while the melting point is high, the recommended maximum operating temperature for nickel crucibles is typically around 700°C (1292°F).

Welded Nickel Rectangular Crucible suppliers

 

Nickel Crucibles Common Applications:

 

Metallurgy:

Nickel crucibles are commonly used for the preparation and analysis of metal alloys. They are suitable for melting, casting, and alloying operations.

01

Ashing:

These crucibles are employed in ashing processes to combust organic matter and leave behind inorganic residues for further analysis.

02

Gravimetric Analysis:

Nickel crucibles are preferred for gravimetric analysis techniques, where precise measurements of sample mass changes are crucial.

03

High-Temperature Reactions:

Researchers use these crucibles to conduct high-temperature chemical reactions, synthesis, and thermal decomposition experiments.

04

Materials Science:

In materials science research, nickel crucibles are instrumental for studying the properties and behaviors of materials under extreme conditions.

05

 

 

Packaging and Shipping

 

 

Packaging

Be packed with Standard export plywood case.

Transportation methods

By standard express(such as UPS, DHL, Fedex, TNT); BY Air Cargo; By sea/ocean.

 

 

FAQ

 

 

Q: What is the use of nickel crucible?

A: The crucible is widely used in crystal growth, metal melting, and high-purity alloy preparation across industries like aerospace, semiconductor fabrication, and specialty materials production.

Q: What are nickel crucibles?

A: Nickel crucibles are high-quality metal containers used in sample preparation for analytical applications, particularly in fusion processes.
Nickel crucibles play a crucial role in laboratory settings, especially in fusion sample preparation. These durable and corrosion-resistant containers are designed to withstand high temperatures and harsh chemical environments, making them ideal for preparing samples with flux for X-ray fluorescence (XRF), inductively coupled plasma (ICP), and other analytical techniques. Their compatibility with various flux materials ensures accurate and reliable sample preparation.

Q: What is the temperature range of a nickel crucible?

A: Nickel Crucibles(Ni Crucibles) Get optimum results with nickel crucibles. With working temperature ranges up to 350°C, the crucible has a high resistance to strong alkalis and phosphoric acid.

We're professional nickel crucibles manufacturers and suppliers in China, featured by quality products and good price. Please rest assured to buy nickel crucibles for sale here from our factory. For customized service, contact us now.

(0/10)

clearall