Titanium Fasteners and Titanium Machined Parts
Standard Titanium Bolts&Nuts in Stocks. Offering Custom Machining Non-standard Parts.
-
Titanium Alloy Motorcycle Oil Cap Screws M121.Titanium alloy motorcycle oil cap screws M122.Material:Titanium Grade 2,Grade 5(TI6AL4V)3.Size:M2/M2.5/M3/M4/M5/M6/M8/M10/M12/M14/M164.Thread pitch:Standard coarseAdd to Inquiry
-
Precision Machined Grade 2 Titanium Stepped ShaftsPrecision Machined Grade 2 Titanium Stepped ShaftsMaterial:CP Grade 2,Grade 3;Titanium alloy Grade 5,Grade 7,Grade 12,etcType:Machined & Drilled, PolishedSize:Can produce according to customer designAdd to Inquiry
-
TI6AL4V Titanium Alloy Pan Head BoltsTI6AL4V Titanium alloy Pan head boltsMaterial:CP Titanium Grade 2,Titanium alloy Grade 5Type:Pan-head boltsThreads:Full threadingFinish:PVD black,Gold; Anodizing colors availableMOQ: 5pcsAdd to Inquiry
-
Multipurpose Titanium Alloy Bolts AnodizedMultipurpose Titanium Alloy Bolts AnodizedMaterial:CP titanium Gr2,Gr3;Titanium alloy Gr5,Gr7,Gr9,Gr12,Gr23,etcStandard:DIN,ISO,JIS,ENSpecs:M1.5-M25* LengthCustom size are accpetableAdd to Inquiry
-
Grade 5 Titanium Alloy Slotted Set Screws With Flat PointGrade 5 Titanium alloy Slotted set screws with flat pointMaterial:CP Titanium Gr1, Gr2;Titanium alloy Gr5, Gr7,Gr9,Gr12Finish:Machined;Polished;Anodized;PVD coatedStandard:DIN 551,ISO 4766,ASMEAdd to Inquiry
-
Titanium Damascus CNC Milling PartsTitanium Damascus CNC milling partsMaterial:Titanium damascus, MokutiCustom CNC Machining: Precision machining based on customer CAD drawings or 3D models,with tolerances±0.02 mmSurfaceAdd to Inquiry
-
Titanium Spring Washers DIN127Titanium Spring Washers DIN127Material:CP titanium Grade 2, Titanium alloy Grade 5Specs:M3/M4/M5/M6/M8/M10/M12/M14/M16/M20Surface Finishes: Natural/Electrolytic Polishing/Passivation/ColoredAdd to Inquiry
-
DIN931 Titanium Hexagon Head BoltsItem name:DIN931 Titanium Hexagon head boltsMaterial:Titanium Grade 2,Grade 5,Grade 7,Grade 9,Grade 12,etcStandard:DIN931/ISO4014,DIN933/ISO4017Specs:M1.5–M64*LengthCustomizationAdd to Inquiry
-
DIN912 Titanium Socket Head Cap Screws M6 M8Item name:DIN912 titanium socket head cap screws M6 M8Material:Titanium Grade2, Grade5, Grade7, Grade 9,Grade 12,Grade 23Specs:M1.5~M24*LengthFinish:Polished,PVD Gold,Blacl,Anodizing Gree PurpleAdd to Inquiry
-
CNC Titanium Alloy Bicycle SprocketItem name:CNC Titanium alloy Bicycle SprocketMaterial:Aerospace titanium alloy Ti-6Al-4VProduction method:Forging+CNC MillingFinish:Polished,Sandblasted,PVD,AnodizingSize:Can be customizedMOQ: 1pieceAdd to Inquiry
-
Grade 5 Titanium Replacement Bolts For MotorcycleGrade 5 titanium replacement bolts for motorcycleMaterial:Grade 5(TI6AL4V),Gr9,etc,Size:M1.5-M15mm*lengthFinish:Polished,Anodized,Sandblast,PVDFeature:Custom size and finishAdd to Inquiry
-
M10x70 Titanium hexagon head tapping screwsM10x70 Titanium hexagon head tapping screwsMaterial:Titanium Gr1,Gr2,Gr3;Titanium alloy Gr5,Gr7,Gr9,Gr12,Gr23,etcScrew feature:Hexagon head+self-tappingAdd to Inquiry
- Baoji Reliab Metal Materials Co.,Ltd
- Mobile:+8613092900605
+8613092913521 - E-mail:garychen3215@hotmail.com
boantj@163.com - Web:www.reliabmetal.com
- Address:No.35 Middle of Baoti Road, Hi-Tech Development Zone, Baoji city, Shaanxi province China 721000
Why Choose Us
Professional Team
The company has more than 110 production workers and more than 35 R&D personnel, forming an experienced and technically solid professional team.
Quality Control
Our products meet international standards such as ASTM F67 and ASTM F136 to ensure stable and reliable product quality.
Advanced Equipment
We are equipped with a series of advanced production equipment, including VAR vacuum melting furnace, 4500T hydraulic press, 800T fast forging press, vacuum annealing furnace, grinder, vertical lathe, three-axis machining center and five-axis machining center.
Sales Market
Our products are exported to many countries and regions such as the United States, the United Kingdom, Germany, France, Japan, Italy, Russia, South Korea, Thailand, the Philippines, Singapore, Poland, Australia, India, New Zealand and Mexico.
Titanium Fasteners and Titanium Machined Parts Specification
|
Physical Properties |
|||
|
Density |
4.51g/cc |
0.163 lb/in³ |
|
|
Mechanical Properties |
|||
|
Hardness, Brinell |
334 |
334 |
Estimated from RockwellC |
|
Hardness,Knoop |
363 |
363 |
Estimated from RockwellC |
|
Hardness, Rockwell C |
36 |
36 |
|
|
Tensile Strength, Ultimate |
950 Mpa |
138000 psi |
|
|
Tensile Strength, Yield |
880 Mpa |
128000 psi |
|
|
Elongation at Break |
14% |
14% |
|
|
Charpy Impact |
17 J |
12.5 ft-lb |
V-notch |

Advantages of Titanium Fasteners and Titanium Machined Parts
Chemical Inertness:
Titanium fasteners and titanium machined parts is durable in many corrosive environments, including exposure to seawater, acids, and various chemicals. This durability is a result of the protective oxide layer, which remains stable under a wide range of corrosive conditions.
Resistance to Pitting Corrosion:
Titanium fasteners and titanium machined parts's resistance to pitting corrosion, a form of corrosion that can lead to small pits or holes in the material, is remarkable. This property is crucial in applications where the fasteners are exposed to harsh conditions, such as in marine environments or chemical processing.
High Temperature Corrosion Resistance:
Titanium fasteners and titanium machined parts retains its corrosion resistance even at elevated temperatures, some up to 315°C, making it suitable for applications where fasteners are exposed to high heat, such as in aerospace and industrial settings.
Galvanic Corrosion Resistance:
Titanium grade metals are excellent at resisting galvanic corrosion, a type of corrosion that occurs when two conductive metals are in contact with an electric current created through chemical action. This makes titanium fasteners and titanium machined parts compatible for use in assemblies with different metals, without significant risk of corrosion.
Biocompatibility:
In medical applications, where titanium fasteners and titanium machined parts may be used in implants, anatomical structures or surgical instruments, the biocompatibility of titanium is a crucial aspect. The corrosion resistance of titanium ensures the longevity and safety of these medical devices within the human body.
Titanium Fasteners and Titanium Machined Parts Grades Chart
|
Grade |
UTS (MPA) |
0.2% (MPA) |
%EL |
O2 %WT |
C %WT |
N %WT |
H %WT |
FE %WT |
|
1 |
240 |
138 |
24 |
0.18 |
0.08 |
0.03 |
0.015 |
0.20 |
|
2 |
345 |
275 |
20 |
0.25 |
0.08 |
0.03 |
0.015 |
0.30 |
|
3 |
450 |
380 |
18 |
0.35 |
0.08 |
0.05 |
0.015 |
0.30 |
|
4 |
550 |
483 |
15 |
0.40 |
0.08 |
0.05 |
0.015 |
0.50 |
|
5 |
950 |
880 |
15 |
0.20 |
0.08 |
0.05 |
0.015 |
0.40 |
Applications of Titanium Fasteners and Titanium Machined Parts
Aerospace Industry: Titanium fasteners and titanium machined partss are extensively used in the aerospace industry due to their high strength and lightweight properties. They are found in aircraft components, including structural parts, engine assemblies, and landing gear.
Medical and Healthcare: Titanium fasteners and titanium machined partss are crucial in the medical field for surgical implants, including bone plates, screws, and dental implants. Their biocompatibility ensures they can be safely used within the human body.
Marine Applications: In the marine industry, titanium fasteners and titanium machined partss are employed in shipbuilding and offshore structures due to their resistance to saltwater corrosion. They are used in critical components like hulls, propellers, and offshore drilling equipment.
Chemical Processing: Titanium fasteners and titanium machined partss are a popular choice in chemical processing plants, where they are used in pipelines, tanks, and equipment that handle corrosive chemicals.
Automotive Industry: The automotive industry benefits from titanium fasteners and titanium machined partss in applications where reducing vehicle weight is essential for improved fuel efficiency and performance.
Sports Equipment: Titanium fasteners and titanium machined partss are used in the production of high-performance sports equipment such as racing bicycles and lightweight sports cars, enhancing durability while minimizing weight.
We have the stocks for most of the normal sizes/specs for different grades of titanium bolts/screws, and can make to order for special sizes according to the design and drawings.
- Stock grades: Gr1, Gr2, Gr5(TI-6AL-4V), Gr7(Ti-0.2Pd), Gr9(Ti-3Al-2.5v), Gr23(Ti-6Al-4V Eli)
- Standard: DIN,ISO,GOST
- Head type of the fasteners: Hexagon head bolts, Cylindrical head hex socket bolts, Torx Socket head Bolts, Flange head bolts, Slotted countersunk screw, Hexagon socket countersunk screw
- Size:M1.5,M2,M2.5,M3,M4,M5,M6,M8,M10,M12,M16,M20,M25,M30
- Colors can make: Blue, Yellow, Purple, Black, Green, Rainbow color, titanium original color.
- MOQ: 1piece for stocks; 100pcs for non-standard spec.
- Logo: Can laser etch Logo or markings.
- Devery time: 5-10days

Packaging and Shipping
|
Packaging |
Be packed with Standard export plywood case. |
|
Transportation methods |
By standard express(such as UPS, DHL, Fedex, TNT); BY Air Cargo; By sea/ocean. |
Trade Terms
|
Payment methods |
T/T, L/C, Credit Card, Paypal, Western Union |
|
Trade terms |
FOB, CIF, C&F, DDP |
|
Delivery time |
3~15 days |
FAQ
We're professional titanium fasteners and titanium machined parts manufacturers and suppliers in China, featured by quality products and good price. Please rest assured to buy titanium fasteners and titanium machined parts for sale here from our factory. For customized service, contact us now.