Titanium Plate
Your Professional Titanium Plate Supplier!
Baoji Reliab Metal Materials Co.,Ltd has focused on top-quality titanium/nickel mill products and titanium alloy machined parts for over 12 years in China. We are one of the leading suppliers in China's titanium and nickel products industry. Our main products include: titanium/nickel bars, plates, tubes, forgings, fasteners, and CNC machined parts.
-
ISO 5832 Medical Titanium SheetISO 5832 Medical Titanium sheetMaterial: CP Grade 3,Grade 4;Alloy Grade 5,Grade 23Standard:ASTM F67,ASTM F136,ISO 5832-2,ISO 5832-3Size:Thickness 0.5mm-60mmWidth:Less than 2000mmLength:Less thanAdd to Inquiry
-
Precision Titanium Soldering Strips PlatesPrecision Titanium Soldering Strips platesMaterial:CP titanium Gr1,Gr2,Gr3;Titanium alloy Gr5,Gr7,Gr9,Gr12Size:Width >5mm,Length Features:Custom size and specsMOQ:1 pieceAdd to Inquiry
-
Grinding Finish Titanium Alloy Plates Ti6Al4VGrinding finish titanium alloy plates Ti6Al4VMaterial:CP Titanium Gr1,Gr2,Titanium alloy Gr5,Gr7,Gr9,Gr12,Gr23Standard:ASTM B265,ASTM F136,AMS 4911Thickness:0.5mm-70mmWidth:Less thanAdd to Inquiry
-
Titanium Chopping Board For KitchenTitanium chopping board for kitchenMaterial:CP Titanium Grade 1,Purity >99.5Thickness:1.5mm,2.0mm,2.5mm,3.0mmSurface:Grinded,PolishedRemarks:Custom specs and sizesMOQ:1pieceAdd to Inquiry
-
Titanium Damascus BilletTitanium Damascus BilletTexture Type:Twisted,Water drop,Rose,Stripe,etcFeatures:Lightweight,Strong,and corrosion-resistantSize:Can be customizedMOQ:1pieceAdd to Inquiry
-
Various Sizes Titanium Element Cube1.Various Sizes titanium element cube2.Material:Titanium Grade 1,Grade 2,Titanium Grade 5(Ti-6Al-4V)3.Size:10*10*10mm,25.4*25.4*25.4mm,31.75*31.75*31.75mm,50.8*50.8*50.8mm,etc4.Finish:SandAdd to Inquiry
-
High Purity Titanium Metal CubeHigh purity titanium metal cube refers to a metal block precision-machined into a regular cube using pure titanium or titanium alloys as raw materials. It is not a single product but encompassesAdd to Inquiry
-
Titanium Bipolar Plates For Hydrogen Production Electroly...1.Titanium bipolar plates for hydrogen production electrolysers2.Material:CP Titanium Grade 1,Grade 23.Thickness:Typically 0.1–0.4 mm4.Accept custom size and specsAdd to Inquiry
-
Bending Titanium Sheet Metal1.Bending titanium sheet metal2.Material:CP titanium Gr1,Gr2;Titanium alloy Gr53.Shape and size can be customized(OEM & ODM)4.Finish:Sand blast;Acid washing;Anodizing5.MOQ:1piece6.Feature:Custom sizeAdd to Inquiry
-
4x8ft Titanium Sheet1.4x8ft Titanium sheet2.Material:Industrial grade pure titanium sheets(such as Gr1 and Gr2)and titanium alloy sheets(such as Gr5/Ti-6Al-4V,Ti-15333,etc.)3.Standard:ASTM B265,AMS 4911,ASTM F136,ASTMAdd to Inquiry
-
Hot Rolled Grade 5 Titanium Alloy PlatesItem name:Hot rolled Grade 5 titanium alloy platesCommonly used grades:Add to Inquiry
-
Gr5 Titanium Alloy Square StripsItem name:Gr5 Titanium alloy square stripsMaterial:Titanium alloy Grade 5, TI6AL4VSize:Width 2mm~50mmLength:Features:Lightweight, high strength, and corrosion resistantAdd to Inquiry
- Baoji Reliab Metal Materials Co.,Ltd
- Mobile:+8613092900605
+8613092913521 - E-mail:garychen3215@hotmail.com
boantj@163.com - Web:www.reliabmetal.com
- Address:No.35 Middle of Baoti Road, Hi-Tech Development Zone, Baoji city, Shaanxi province China 721000
Why Choose Us
Professional Team
The company has more than 110 production workers and more than 35 R&D personnel, forming an experienced and technically solid professional team.
Quality Control
Our products meet international standards such as ASTM F67 and ASTM F136 to ensure stable and reliable product quality.
Advanced Equipment
We are equipped with a series of advanced production equipment, including VAR vacuum melting furnace, 4500T hydraulic press, 800T fast forging press, vacuum annealing furnace, grinder, vertical lathe, three-axis machining center and five-axis machining center.
Sales Market
Our products are exported to many countries and regions such as the United States, the United Kingdom, Germany, France, Japan, Italy, Russia, South Korea, Thailand, the Philippines, Singapore, Poland, Australia, India, New Zealand and Mexico.
Titanium Plate Specification
|
Physical Properties |
|||
|
Density |
4.51g/cc |
0.163 lb/in³ |
|
|
Mechanical Properties |
|||
|
Hardness, Rockwell B |
98 |
98 |
|
|
Shear Modulus |
38 MPa |
5510 ksi |
|
|
Shear Strength |
380 MPa |
55100 psi |
|
|
Tensile Strength, Ultimate |
430 MPa |
62400 psi |
|
|
Tensile Strength, Yield |
340 MPa |
49300 psi |
|
|
Elongation at Break |
28% |
28% |
|
|
Charpy Impact |
65 J |
47.9 ft-lb |
V-notch |
Advantages of Titanium Plate
Exceptional Strength-to-Weight Ratio
One of the most significant benefits of using titanium plates is their exceptional strength-to-weight ratio.Despite being lighter, titanium is incredibly strong.
Corrosion Resistance
Titanium plate is highly resistant to corrosion, which is another reason why titanium plates are so widely used. The metal forms a thin oxide layer on its surface when exposed to oxygen, which protects it from corrosion.
Biocompatibility
Titanium plate is one of the few metals that is fully biocompatible, meaning it does not cause adverse reactions when implanted in the human body.
High Temperature Resistance
Another key advantage of titanium plates is their ability to withstand high temperatures. Titanium can maintain its strength and integrity at temperatures that would cause other metals to weaken or fail.
Low Thermal Expansion
Titanium plate has a low coefficient of thermal expansion, which means it does not expand or contract significantly with changes in temperature.
Versatility in Form and Application
Titanium plates are extremely versatile and can be used in a wide range of applications. They can be easily fabricated into various shapes and sizes to meet specific requirements.
Titanium Plate Chemical Composition
|
Symbol |
Element |
Min % |
Max % |
|
Al |
Aluminum |
5.50% |
6.75% |
|
V |
Vanadium |
3.50% |
4.50% |
|
Fe |
Iron |
|
0.30% |
|
O |
Oxygen |
|
0.20% |
|
C |
Carbon |
|
0.08% |
|
N |
Nitrogen |
|
0.05% |
|
H |
Hydrogen |
|
0.01% |
|
Y |
Yttrium |
|
0.01% |
|
|
Other, each |
|
0.10% |
|
|
Other, total |
|
0.40% |
|
Ti |
Titanium |
|
Remainder |

Application of Titanium Plate
Aerospace industry:
Used in the manufacture of aircraft structural components, engine components and spacecraft components, using its excellent strength-to-weight ratio to reduce the weight of aircraft, and improve fuel efficiency and performance.
Chemical industry:
Used in the manufacture of corrosion-resistant chemical equipment, such as reactors, vessels and pipelines, due to its excellent corrosion resistance, can withstand a variety of corrosive media erosion.
Marine Engineering:
Used in the manufacture of offshore platforms, ship components desalination equipment, etc., which can be used in the marine environment for a long time due to its ability to resist seawater corrosion.
Medical devices:
Used in the manufacture of medical implants, such as artificial joints, dental implants, etc., because of their good biocompatibility, do not easy to cause rejection of the human body.
Automotive industry:
Used in the manufacture of automotive exhaust systems, chassis components and body structures, the use of its lightweight and high-strength characteristics, to improve automotive performance and fuel efficiency.
We have the stocks for most of the normal sizes/specs for different grades of titanium and titanium alloy, and can make to order for special sizes.
- Stock grades: Gr1, Gr2, Gr5(TI-6AL-4V), Gr7(Ti-0.2Pd), Gr9(Ti-3Al-2.5v), Gr23(Ti-6Al-4V Eli)
- Standard: ASTM B265, AMS 4911
- Surface: Milled, Ploshed ,Pickling surface
- Size of stocks:δ0.5mm,δ1mm,δ1.5mm,δ 2mm, δ2.5mm, δ 3mm, δ3.5mm, δ 4mm, δ4.5mm, δ5mm, δ5.5mm, δ6mm, δ6.5mm, δ7mm, δ8mm, δ8.5mm, δ9mm, δ9.5mm, δ10mm, δ12mm, δ14mm, δ15mm, δ16mm, δ18mm, δ20mm, δ25mm, δ28mm, δ30mm, δ35mm, δ40mm, δ45mm, δ50mm...
- Width: 0~1300mm
- Length: 0~6000mm

Packaging and Shipping
|
Packaging |
Be packed with Standard export plywood case. |
|
Transportation methods |
By standard express(such as UPS, DHL, Fedex, TNT); BY Air Cargo; By sea/ocean. |
Trade Terms
|
Payment methods |
T/T, L/C, Credit Card, Paypal, Western Union |
|
Trade terms |
FOB, CIF, C&F, DDP |
|
Delivery time |
3~15 days |
FAQ
We're professional titanium plate manufacturers and suppliers in China, featured by quality products and good price. Please rest assured to buy titanium plate for sale here from our factory. For customized service, contact us now.
titanium gold price, titanium foil, 1 gram titanium price