Definition of Titanium bolts for motorcycle rearview mirror M8
Titanium bolts for motorcycle rearview mirror M8 M10 are high-performance fasteners featuring Grade 5 (TC4/6Al-4V) titanium alloy as their core material. They emphasize lightweight construction, high strength, corrosion resistance, and aesthetic appeal, making them the mainstream choice for motorcycle rearview mirror modifications and performance upgrades.
Though small, titanium rearview mirror screws serve as a cost-effective upgrade in motorcycle customization, combining functionality (lightweight, durable) with aesthetics (titanium-colored finish). For detail-oriented riders, this represents a wise choice-a one-time investment yielding long-term benefits.
Material and Grade of Titanium bolts for motorcycle rearview mirror M8
Motorcycle rearview mirror titanium screws primarily utilize Grade 5 titanium alloy, specifically Ti-6Al-4V (titanium alloy with 6% aluminum and 4% vanadium). This aerospace-grade titanium alloy material possesses the following characteristics:
Titanium (Ti) 90% + Aluminum (Al) 6% + Vanadium (V) 4% is the standard high-strength titanium alloy used in aerospace and high-end machinery applications.
Density: 4.51 g/cm³, approximately 45-50% lighter than steel
Tensile strength: 895-1100 MPa, nearly double that of 316 stainless steel (570 MPa)
Corrosion resistance: Forms a natural oxide layer on the surface, preventing rust in humid and salt spray environments
Temperature resistance: Excellent high-temperature and low-temperature performance
Common Specifications and Dimensions
|
Thread size |
Common Length |
Applicable Vehicle Models/Locations |
Head Type |
|---|---|---|---|
| M6 | 15-25mm |
Rearview mirrors for small motorcycles and electric vehicles |
Hex socket head cap screws, Torx-head screws |
| M8 | 15-35mm |
Mainstream Japanese/domestic models (such as Yamaha, Honda) |
Flange head, round head, disc head |
| M10 | 15-40mm |
Large-displacement vehicles, heavy-duty rearview mirror mounts |
Internal flower-head, twelve-pointed head |
| M12 | 20-50mm |
Special modification parts, extension brackets |
Flange-face bolts |
Special Design:
- Left/Right Threads (Right-Hand/Left-Hand): Certain models require left-hand threads to prevent rearview mirrors from loosening due to driving vibrations.
- Adapter Screws: M8-to-M10 or similar size conversion screws, used to adapt mirrors of different specifications.
Mainstream Specifications (Metric)
- M8: Pitch P1.25, common lengths 15/20/25/30/35 mm, individual weight approx. 4.8–7 g.
- M10: Pitch P1.25 (mainstream)/P1.5, common lengths 15/20/25/30/35 mm, individual weight approx. 7.3–10 g.
Surface Treatment and Color of Titanium bolts for motorcycle rearview mirror M8
Titanium screws can be finished in various colors through PVD coating or anodizing to meet aesthetic customization needs:
- Burned titanium/rainbow colors: Oxidation hues formed by high-temperature treatment, the most popular custom style
- Gold, blue, purple, black: Achieved via anodizing or PVD coating
- Natural/silver: Polished or acid-washed to reveal the base metal's color
- Dual-tone combinations: Such as gold-blue, blue-purple, etc.
Core Competitive Advantages of Titanium bolts for motorcycle rearview mirror M8
1. Ultimate Lightweight Design
40-50% lighter than steel screws of the same specification. For race cars or modified vehicles pursuing extreme weight reduction, a full titanium screw conversion can shed hundreds of grams of unsprung mass.
2. Permanent Corrosion Resistance
Never rusts in harsh environments like rain, mud, or salt-coated roads, making it ideal for coastal regions or vehicles frequently parked outdoors.
3. Vibration Fatigue Resistance
Titanium alloy's moderate elastic modulus effectively absorbs vibrations transmitted from engines and road surfaces, preventing screw loosening and offering greater durability than standard steel screws.
4. High-Strength Assurance
Grade 5 titanium alloy achieves a strength rating of 10.9, ensuring mirror stability during high-speed driving.
5. Aesthetic Modification Value
The unique burnished titanium finish significantly elevates vehicle sophistication, making it a popular choice for exterior upgrades.
Products showcase of Titanium bolts for motorcycle rearview mirror M8
Titanium bolts for motorcycle rearview mirror M8






how to contact us
E-mail: garychen3215@hotmail.com
Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China
Contact: Mr. Gary Chen
Phone: +86-917-8883215
Mobile/WhatsApp: +86 13092900605
Hot Tags: Titanium Bolts For Motorcycle Rearview Mirror M8, China Titanium Bolts For Motorcycle Rearview Mirror M8 manufacturers, suppliers, factory, custom titanium fasteners, titanium sheet, race bolts titanium bolts, 1kg titanium price, m14 titanium bolt, PVD TI6AL4V Torx Bolts for Motors