Titanium tubes (commonly made of Gr2 or Gr5) are much more difficult to cut than ordinary steel tubes due to their high toughness, low thermal conductivity, susceptibility to oxidation, and tendency to stick to the blade; the key to successful cutting lies in temperature control, preventing oxidation and deformation, and deburring.

Below, we will analyze several common methods for cutting titanium tubes:

1. Band Saw Machine / Horizontal Metal Band Saw

Applications: Φ10–Φ200mm, wall thickness 1–20 mm, for batch cutting

Key Parameters:

Linear Speed: 15–35 m/min (Low speed! Titanium has poor thermal conductivity; high speeds cause tool burning and sticking)

Feed Rate: Light feed (0.05–0.1 mm/tooth)

Must use ample emulsion or specialized cutting fluid (for cooling and anti-welding)

Tubes must be securely clamped and internally supported (thin-walled tubes are prone to ovalization and tool vibration)

Advantages: Low-cost equipment, smooth cut surface, no heat-affected zone, minimal deformation

Disadvantages: Slow speed, moderate burr formation

2. Grinding Wheel Cutting / Pipe Cutter (Fast rough cutting; commonly used on-site)

Applications: Small quantities on-site; diameter ≤ 100 mm; wall thickness ≤ 8 mm; low-precision requirements

Grinding Wheels: Resin-bonded grinding wheels; stainless steel-specific / titanium-specific (high-alumina, ferrite-free)

Speed: Low speed (2000–3000 rpm)

Continuous water cooling (titanium is prone to oxidation, discoloration, embrittlement, and blueing at high temperatures)

Make a single cut; do not saw back and forth repeatedly

Remove the oxide layer and deburr after cutting

3. Fiber Laser Tube Cutting (High Precision, Thin-Walled, Batch Production)

Applications: Φ20–Φ200, wall thickness 0.5–6 mm, precision parts / welded components

Parameters:

Machine Type: Fiber laser 1–3 kW

Assist Gas: High-purity argon / nitrogen (Oxygen strictly prohibited! Titanium has a low ignition point and is prone to ablation and oxidation)

Heat-Affected Zone: <100 μm, virtually no deformation

Accuracy: ±0.05–0.1 mm

Advantages:

Smooth, burr-free cut; excellent perpendicularity; capable of cutting bevels

Suitable for thin-walled titanium tubes (≤2 mm) with minimal risk of collapse

Disadvantages: Expensive equipment; low efficiency for thick-walled tubes (>8 mm)

Gr5 titanium tubingTitanium round pipe supplier

product-78-67 Website: www.reliabmetal.com

product-72-64 Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

product-72-69 Contact: Mr. Gary Chen

product-67-66 Phone: +86-917-8883215

product-71-72 Mobile/WhatsApp: +86 13092900605

product-72-64 E-mail: garychen3215@hotmail.com

 

Send Inquiry
Contact Us
    • Baoji Reliab Metal Materials Co.,Ltd
    • Mobile:+8613092900605
                     +8613092913521
    • E-mail:garychen3215@hotmail.com
                     boantj@163.com
    • Web:www.reliabmetal.com
    • Address:No.35 Middle of Baoti Road, Hi-Tech Development Zone, Baoji city, Shaanxi province China 721000