ASTM B348 Titanium Round Bar
video
ASTM B348 Titanium Round Bar

ASTM B348 Titanium Round Bar

Brand Name: RLD
Application:S emiconductor, Petroleum
Shape: Round, Squre
Length: 10~6000mm
Standard: ASTM B348 AMS4928 AMS 4911 ASTM F136
Certificate: ISO 9001: 2015 EN 1024 3.1 EN 1024 3.2
Surface: Polishing,Grinding
Send Inquiry
Description

Introduction of titanium round bars

 

Product Name

ASTM B348 Titanium round bar

Material

Gr1,Gr2,Gr3,Gr4,Gr5(Ti-6Al-4V),Gr7,Gr9,Gr11,Gr12,Gr23(Ti-6Al-4V Eli),Gr28

Standard

ASTM B348, F67, F136, AMS4928,AMS4967,AMS4931

Specification

Round bar: Dia(6-300) *Lmm or as customized

Hex bar : SW(4-100)*Lmm or as customized
Squarer bar: W(6-100)*TK(6-100)*Lmm

Surface

Polished,machined,peeled

Product Type

Round, Square, hexagonal

Certification

AS9100D,NORSOK M650 PED 4.3

Technique

Hot rolled or cold rolled

Application

Chemical industry
Petrochemical industry
Machining field,Automobile field,etc.
Textile printing and dyeing
industry, and so on.

Quality and Test

test and inspections ensure the materials meet destructive and non-destructive test according to industry and customers specifications.

 

Manufacturing process of titanium round bars

 

image001

Material Data of ASTM B348 Titanium round bar

 

Gr5

Metric

English

Remarks

Physical Properties

Density

4.51g/cc

0.163 lb/in³

 

Mechanical Properties

Hardness, Brinell

334

334

Estimated from RockwellC

Hardness,Knoop

363

363

Estimated from RockwellC

Hardness, Rockwell C

36

36

 

Tensile Strength, Ultimate

950 Mpa

138000 psi

 

Tensile Strength, Yield

880 Mpa

128000 psi

 

Elongation at Break

14%

14%

 

Charpy Impact

17 J

12.5 ft-lb

V-notch

 

Picture Showcase of ASTM B348 Titanium round bar

 

image003
image005
image007
image009

 

About our factory

 

Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel,Zirconium products. With high quality controlling system, our products meeting the international standard as ASTM, ASME, AMS, JIS, DIN, TOCT, our main products including bars/rods, plates/sheets, tubes, wires, forgings rings, anodes, fasteners and CNC machined parts.

For over 11 years,Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.

*TO BE YOUR RELIABLE AND TRUSTABLE PARTNER AS ALWAYS!!*

 

Our Company Advantages

 

  • More than 15 years producing titanium bar.
  • Specializing in the production of various titanium bar.
  • Provide customers with titanium products solutions.
  • Superior material and competitive price.
  • Reply your inquiry within 24 hours.

 

About Shipping

 

** By express: DHL, UPS, FEDEX, TNT, SF, Postal express.(around 4~5 days)

** By air cargo (around 5~7 days)

** By sea/ocean (around 12~25 days)

 

image013

Hot Tags: astm b348 titanium round bar, China astm b348 titanium round bar manufacturers, suppliers, factory, ASTM F67 H9 Titanium Bar, titanium tig welding wire, TIG Titanium Welding Rod, titanium necklaces, titanium cost, titanium products