Industrial Grade 2 Titanium Sheet 2mm 3mm
video
Industrial Grade 2 Titanium Sheet 2mm 3mm

Industrial Grade 2 Titanium Sheet 2mm 3mm

Item name:Industrial Grade 2 titanium sheet 2mm 3mm
Thickness: From0.5mm~50mm
Material: CP Titanium Grade 1,Grade 2, Grade3
Status: Cold Rolled,Hot rolled
Standard: ASTM B265, AMS 4911
Send Inquiry
Description

Brief Data of Industrial Grade 2 titanium sheet 2mm 3mm

 

Standard: ASTM B265, AMS 4911

Grade:Grade 1,Grade 2,Grade 3

Manufacturing Processes:Cold Rolling,Hot Rolling

Size:Thickness 0.5mm~50.0mm*Width<1500mm*Length<6000mm

Features: The excellent properties of Titanium Plates include high strength, low density, good mechanical properties, corrosion resistance, high stability and so on. So Titanium & Titanium Alloy Plates always be used in airplane engine components, rockets, missile and other aircraft components.

In addition to that, titanium and titanium alloy plates also can be used in industrial construction , sports equipment, tableware, outdoor supplies and so on. The good performances of titanium plates make it easy to be accept and are more and more familiar by public.

 

Material Data of Industrial Grade 2 titanium sheet 2mm 3mm

 

 

Metric

English

Remarks

Physical Properties

Density

4.51g/cc

0.163 lb/in³

 

Mechanical Properties

Hardness, Rockwell B

98

98

 

Shear Modulus

38 MPa

5510 ksi

 

Shear Strength

380 MPa

55100 psi

 

Tensile Strength, Ultimate

430 MPa

62400 psi

 

Tensile Strength, Yield

340 MPa

49300 psi

 

Elongation at Break

28%

28%

 

Charpy Impact

65 J

47.9 ft-lb

V-notch

 

Rolling Processing of Industrial Grade 2 titanium sheet 2mm 3mm

 

(1)Hot Rolled Processing:

Hot rolling is carried out above the recrystallization temperature of titanium alloys and is suitable for the production of medium-thickness plates (such as those with a thickness of more than 5mm). Hot rolling can enable titanium alloy plates to obtain good internal structure and mechanical properties, and improve the plasticity and toughness of the plates.

(2)Cold Rolled Processing:

Cold rolling is a rolling process carried out at room temperature, and is mainly used for the production of thin plates (such as those with a thickness ranging from 0.3 to 5mm), which can achieve higher surface accuracy and dimensional accuracy. The surface of the cold-rolled titanium alloy sheet is smooth and the thickness is uniform, making it suitable for components with high requirements for the surface quality of the sheet.

(3)Comparison of Rolling Processes:

Hot rolling and cold rolling both have their own advantages and disadvantages.

Hot rolling has a high production efficiency, but its surface quality is relatively poor.

Cold-rolled surfaces have good quality, but the production cost is relatively high.

In actual production, the appropriate rolling process can be selected according to the product requirements.

 

Ten Properties of Industrial Grade 2 titanium sheet 2mm 3mm

 

  • Low Density, High specific strength
  • Excellent corrosion resistance
  • Good heat resistance
  • Good Low temperature performance
  • Strong Anti damping performance
  • Non-magnetic, Non-toxic
  • Small heat conduction coefficient
  • Low modules of elasticity
  • The suction performance
  • Tensile strength close to the yield strength

 

Products Showcase of Industrial Grade 2 titanium sheet 2mm 3mm

 

Industrial Grade 2 titanium sheet 2mm 3mm
Industrial Grade 2 titanium sheet 2mm 3mm supplier
Industrial Grade 2 titanium sheet 2mm 3mm manufacturer
Industrial Grade 2 titanium sheet 2mm 3mm for sale

 

 

About Our Factory

Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel,Zirconium products. With high quality controlling system, our products meeting the international standard as ASTM, ASME, AMS, JIS, DIN, TOCT, our main products including bars/rods, plates/sheets, tubes, wires, forgings rings, anodes, fasteners and CNC machined parts.

For over 11 years, Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.

Industrial Grade 2 titanium sheet 2mm 3mm made in China

 

*TO BE YOUR RELIABLE AND TRUSTABLE PARTNER AS ALWAYS!!*

Hot Tags: industrial grade 2 titanium sheet 2mm 3mm, China industrial grade 2 titanium sheet 2mm 3mm manufacturers, suppliers, factory, cutting titanium, Titanium Thin Sheet for Heat Exchanger, titanium foam, titanium steel, tio2 price, titanium flat bar stock

Send Inquiry

(0/10)