During the process of wheel hub modification, we usually meets two types of wheel hub screws: One is the most common nut type screw, which is more common in Japanese and American cars. Its feature is that it is easy to disassemble; just unscrew the nut. Another type is the specially designed wheel hub screws, which not only have unique aesthetic value but also provide more stable support for the vehicle.
Material Data of Grade 5 Titanium wheel bolt
Material Notes: Alpha-Beta Alloy
|
Metric |
English |
Remarks |
|
|
Physical Properties |
|||
|
Density |
4.51g/cc |
0.163 lb/in³ |
|
|
Mechanical Properties |
|||
|
Hardness, Brinell |
334 |
334 |
Estimated from RockwellC |
|
Hardness,Knoop |
363 |
363 |
Estimated from RockwellC |
|
Hardness, Rockwell C |
36 |
36 |
|
|
Tensile Strength, Ultimate |
950 Mpa |
138000 psi |
|
|
Tensile Strength, Yield |
880 Mpa |
128000 psi |
|
|
Elongation at Break |
14% |
14% |
|
|
Charpy Impact |
17 J |
12.5 ft-lb |
V-notch |
Picture Showcase of the Gr5 Titanium wheel bolt M12 for wheel hub




What benefits can the titanium Gr5 bring to the automotive industry ?
Titanium alloys have the advantages of high strength, corrosion resistance and high-temperature resistance, and thus are widely used in the automotive industry. The following are some benefits that the use of titanium rods can bring to the automotive industry:
1. Weight reduction: Gr5 Titanium wheel bolt M12 for wheel hub are lighter than steel of the same volume. Using them can significantly reduce the overall weight of a car, thereby improving fuel economy and lowering exhaust emissions.
2. Enhance safety: It features high strength and high toughness, which can improve the car's cragging resistance and durability, thereby enhancing the vehicle's safety performance.
3. Enhanced performance: It has excellent mechanical and chemical properties, capable of maintaining stable performance in harsh working environments, thereby enhancing the performance and reliability of the vehicle.
4. Reduce maintenance costs: It has excellent corrosion resistance, which can extend the service life of automotive parts and thereby reduce the maintenance costs of automobiles.
5. Enhance quality: The appearance of titanium rods is bright and the surface is smooth. Using them can enhance the appearance quality and added value of automobiles.
About Shipping
We can ship out the goods by international express(like DHL, UPS, Fedex), Air cargo, and Ocean/sea shipping.

Hot Tags: gr5 titanium wheel bolt m12 for wheel hub, China gr5 titanium wheel bolt m12 for wheel hub manufacturers, suppliers, factory, titanium fasteners in aluminum, titanium bolts for sale, titanium dowel pins, m14 titanium bolt, m3 titanium bolts, titanium alloy fasteners