Part name:M2.5 titanium alloy cylindrical head socket cap screw
Material:Titanium Grade 5(Ti-6Al-4V)
Standard:DIN 912,ISO 4762
Thread specification M2.5×0.45 (coarse thread)
Finish:Machined+Polished
MOQ:10 pcs
Send Inquiry
Description

Definition of M2.5 titanium alloy cylindrical head socket head cap screws

 

M2.5 titanium alloy cylindrical head socket head cap screws are lightweight, high-strength, and corrosion-resistant precision fasteners. The main material is Ti-6Al-4V (Grade 5/TC4), conforming to DIN 912/ISO 4762 standards. The thread specification is M2.5×0.45 (coarse thread). They are widely used in aerospace, precision electronics, medical devices, and other applications where weight and reliability are critical.

 

Core specifications and dimensions

 

Thread specification: M2.5, Nominal diameter: 2.5mm

Thread pitch: 0.45mm (Coarse thread standard (DIN 912), fine thread option: 0.35mm)

Head diameter (D): 4.5 mm +0/-0.18 mm

Head height (H): 2.5 mm +0/-0.14 mm

Hexagonal socket size (J): 2.0mm (Requires a 2.0mm hex wrench)

Head drive depth (P): 1.1 mm (Standard internal hexagon countersink depth)

Nominal length (L) 4~30mm (common) 4/5/6/8/10/12/16/20/25/30mm

Thread length: Full thread / Partial thread; Short lengths are fully threaded, long lengths are partially threaded (according to standard).

Standard: DIN 912 / ISO 4762 General standard for socket head cap screws

 

chemical compositions

 

Ti (Titanium): Excess material | Base material, lightweight, corrosion-resistant

Al: 5.5~6.75 ; Strengthens the α phase, improving strength and heat resistance.

V: 3.5~4.5;  Stabilizes the β phase, improving toughness and weldability.

Fe: ≤0.30 ; Impurities; content is controlled to ensure purity.

C: ≤ 0.08 ; Impurities, to prevent carbide embrittlement.

N: ≤ 0.05 ; Impurities, affecting plasticity

H: ≤ 0.015 ; Impurities, to prevent hydrogen embrittlement

O: ≤ 0.20 ; Impurities; controlling oxygen content ensures ductility.

 

Mechanical properties

 

Tensile strength (σb) ≥ 895 MPa, approximately 1.5 times that of 304 stainless steel.

Yield strength (σ0.2) ≥ 828 MPa High strength, strong resistance to deformation

Elongation (δ5) ≥10% Possesses a certain degree of toughness and is not easily brittle.

Hardness (HRC): 33~38 Medium hardness, wear-resistant and machinable.

Density: 4.51 g/cm³, approximately 57% of stainless steel (7.93 g/cm³), demonstrating a significant advantage in terms of lightweight properties.

Temperature resistance: -196~300℃ (Suitable for long-term use at ≤300℃, and can withstand higher temperatures for short periods.)

Corrosion resistance: Excellent; resistant to atmospheric conditions, seawater, acids and alkalis (non-strong oxidizing agents), non-magnetic.

Non-magnetic: Suitable for medical equipment, precision electronics, and magnetic-sensitive applications.

Biocompatibility: Grade 5 titanium alloy can be used in implantable medical devices (additional surface treatment required);

Surface treatment: Natural finish (acid pickling/passivation), anodizing (colored, improves wear resistance and insulation), chemical polishing (high cleanliness, suitable for semiconductor/medical applications);

 

Production process

 

  1. Raw Materials: Ti-6Al-4V bar stock (Grade 5), inspected, straightened, and peeled to ensure no defects;
  2. Cold Heading: Using a multi-station cold heading machine, the cylindrical head and internal hexagonal hole are formed in one step, ensuring dimensional accuracy and density of the head;
  3. Thread Machining: Thread rolling (full thread) or thread cutting (partial thread), thread accuracy 6g, smooth surface, no burrs;
  4. Heat Treatment: Solution treatment + aging (β annealing + aging) to improve strength and toughness and eliminate processing stress;
  5. Surface Treatment: Pickling and passivation (to remove oxide scale and form a passivation film), anodizing (optional), chemical polishing (cleanroom grade);
  6. Inspection: 100% dimensional inspection (caliper/projector), mechanical property sampling inspection (tensile strength/hardness), salt spray test (corrosion resistance), non-destructive testing (critical parts);
  7. Packaging: Anti-static bags/clean boxes, suitable for export and precision equipment assembly.

 

Application Scenarios (Core Areas)

 

  • Aerospace: Structural components and electronic compartment fasteners for drones, satellites, and aircraft models; crucial for lightweighting and weight reduction;
  • Precision Electronics: Internal fasteners for mobile phones, laptops, cameras, and servers; features include non-magnetic properties, lightweight design, and corrosion resistance;
  • Medical Devices: Surgical instruments, implantable device components, and medical equipment casings; features include biocompatibility and corrosion resistance;
  • Automotive Modification: Lightweight components for racing cars and new energy vehicles; weight reduction improves performance;
  • Semiconductor/Optoelectronics: FPD (Flat Panel Display) manufacturing equipment, semiconductor packaging equipment; features include cleanliness, non-magnetic properties, and corrosion resistance;
  • Outdoor/Marine: Photographic equipment, outdoor gear, and precision components for ships; features include seawater corrosion resistance and lightweight design.

 

Products pictures show of M2.5 titanium alloy cylindrical head socket cap screw

 

M2.5 titanium alloy cylindrical head socket cap screw
M2.5 titanium alloy cylindrical head socket cap screw factory
M2.5 titanium alloy cylindrical head socket cap screw
M2.5 titanium alloy cylindrical head socket cap screw in stocks

FAQ

 

Q: How does this M2.5 titanium alloy cylindrical head socket cap screw was manufactured?

A: Briefly speaking, M2.5 titanium alloy cylindrical head socket cap screw was hot-forged==>machined==>polished.

 

Q: Can you make LOGO on the M2.5 titanium alloy cylindrical head socket cap screw?

A: We can laser engraving customers logo for free.

 

Q: What is the MOQ on the M2.5 titanium alloy cylindrical head socket cap screw?

A: Our MOQ on the M2.5 titanium alloy cylindrical head socket cap screw is 10 pcs.

 

how to contact us

 

M2.5 titanium alloy cylindrical head socket cap screw E-mail: garychen3215@hotmail.com

M2.5 titanium alloy cylindrical head socket cap screw Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

M2.5 titanium alloy cylindrical head socket cap screw Contact: Mr. Gary Chen

M2.5 titanium alloy cylindrical head socket cap screw Phone: +86-917-8883215

M2.5 titanium alloy cylindrical head socket cap screw Mobile/WhatsApp: +86 13092900605

 

Hot Tags: m2.5 titanium alloy cylindrical head socket cap screw, China m2.5 titanium alloy cylindrical head socket cap screw manufacturers, suppliers, factory, bolts, titanium suppliers, titanium wood screws, anodized titanium bolts, titanium bolts price, titanium bolts for sale

Send Inquiry

(0/10)

clearall