What is Titanium Grade 2 Full Threaded Hex Bolt?
Titanium Grade 2 Full Threaded Hex Bolt are fasteners made of titanium alloys (such as Gr2 and Gr5), renowned for their lightweight, high strength (tensile strength exceeding 895 MPa), and excellent corrosion resistance. They are widely used in high-end fields such as aerospace, medical, chemical, and marine industries.
Their core advantages are:
Lightweight: With a density of only 4.5 g/cm³, it is approximately 40% lighter than steel, effectively reducing equipment weight.
High Strength: Gr5 titanium alloy has strength comparable to 10.9 grade high-strength steel, but with a higher specific strength.
Corrosion Resistance: The surface passivation film makes it perform excellently in acidic, alkaline, saline, and marine environments, resulting in a long service life.
Specifications of Titanium Grade 2 Full Threaded Hex Bolt
Titanium Grade 2 Full Threaded Hex Bolts come in a wide range of sizes, from M3 to M20, with M4, M5, M6, M8, M10, M12, M14, M16, M18, and M20 being the most common standard sizes. These sizes are typically expressed as "diameter × length," such as M415 and M520, with lengths ranging from a few millimeters to hundreds of millimeters to meet the needs of various industrial applications.
Strength grade of Titanium Grade 2 Full Threaded Hex Bolt
GR2 Titanium Alloy
Tensile Strength: 400-550 MPa (approx. 480 MPa for cold-rolled sheets, approx. 505 MPa for hot-rolled sheets, forgings up to 530 MPa)
Yield Strength: 230-350 MPa (approx. 270 MPa for cold-rolled sheets, approx. 310 MPa for hot-rolled sheets)
Features: Industrially pure titanium, excellent corrosion resistance, suitable for chemical, marine, and other environments.
GR5 Titanium Alloy
Tensile Strength: ≥895 MPa (some data can reach 1200 MPa)
Yield Strength: ≥800 MPa (ratio to tensile strength approx. 0.9)
Features: α-β type two-phase alloy, containing 6% aluminum and 4% vanadium, combining high strength and corrosion resistance, widely used in aerospace and medical fields.
The highest strength grade for titanium alloy screws is 12.9, with the following performance requirements:
Axial tensile strength: ≥1200 MPa
Axial yield strength: ≥1080 MPa (yield ratio 0.9)
Applicable scenarios: Aerospace, precision machinery, and other fields requiring ultra-high strength.
Products showcase of Titanium Grade 2 Full Threaded Hex Bolt




about us
Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel,Zirconium products. With high quality controlling system, our products meeting the international standard as ASTM, ASME, AMS, JIS, DIN, TOCT, our main products including bars/rods, plates/sheets, tubes, wires, forgings rings, anodes, fasteners and CNC machined parts.
For over 11 years,Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.

contact us
E-mail: garychen3215@hotmail.com
Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China
Contact: Mr. Gary Chen
Phone: +86-917-8883215
Mobile/WhatsApp: +86 13092900605
Hot Tags: titanium grade 2 full threaded hex bolt, China titanium grade 2 full threaded hex bolt manufacturers, suppliers, factory, titanium fairing bolts, Titanium Flange Bolts for Motorcycle, titanium bolts for bikes, m6 bicycle bolts, titanium bolt grades, ti mtb bolts