Gr5 Titanium Seamless Pipes
video
Gr5 Titanium Seamless Pipes

Gr5 Titanium Seamless Pipes

Gr5 Titanium seamless pipes
Material:Titanium Grade 5(Ti-6Al-4V)
Standard:ASTM B337,ASTM B338,ASTM B861
Size:OD10mm-200mm*Length <6000mm
MOQ:1 piece
Send Inquiry
Description

definition About Gr5 Titanium seamless pipes

 

Gr5 Titanium seamless pipes is manufactured from Ti-6Al-4V (titanium-6-aluminum-4-vanadium) alloy and is one of the most widely used titanium alloy tubes in the industry. GR5 is an α-β titanium alloy and is regarded as the "workhorse" of titanium alloys due to its excellent overall performance.

It is the world's most widely used and versatile seamless tube made from an α+β two-phase heat-treatable titanium alloy. With high strength, lightweight properties, excellent corrosion resistance, and good weldability and formability as its core advantages, it is suitable for demanding applications in the aerospace, marine, chemical, medical, and high-end equipment industries.

 

Chemical Composition of Gr5 Titanium seamless pipes

 

Elements Standard Range

Function

Ti

Residual content

Basic element
Al 5.5%–6.75%

α-stabilized, improved strength, heat resistance, and creep resistance

V 3.5%–4.5%

β-stabilization; improved ductility, weldability, and heat treatment hardenability

O ≤0.20%(Standard);≤0.13%(ELI)

Interstitial strengthening; controlling oxygen content to ensure toughness

N ≤0.05%

Interstitial impurities: Strictly control to prevent embrittlement

C ≤0.08%

Impurities, affecting ductility

H ≤0.015%

Strictly control hydrogen to prevent hydrogen embrittlement

 

Ten Properties of Titanium

 

① Low Density, High specific strength

② Excellent corrosion resistance

③ Good heat resistance

④ Good Low temperature performance

⑤ Strong Anti damping performance

⑥ Non-magnetic, Non-toxic

⑦ Small heat conduction coefficient

⑧ Low modules of elasticity

⑨ The suction performance

⑩ Tensile strength close to the yield strength

 

Mechanical Properties of Gr5 Titanium seamless pipes

 

Performance Metrics

Minimum Value

Typical Value

Tensile strength

≥ 895 MPa 930 ~ 970 MPa

Yield strength

≥ 828 MPa 880 ~ 930 MPa

Elongation

≥ 10% 12 ~ 14%

Cross-sectional reduction ratio

≥ 25% 30 ~ 35%
Hardness(HRC) 30 ~ 36 34 ~ 38

 

Specifications of Gr5 Titanium seamless pipes

 

1. Size Range (Outer Diameter × Wall Thickness × Length)

Outer Diameter (OD): Φ10 mm–Φ200 mm (standard: Φ10–Φ108), customizable up to Φ300 mm

Wall Thickness (WT): 1 mm–20 mm (standard: 1–8 mm), thin-walled ≤0.8 mm, thick-walled ≥15 mm

Length: 1000–6000 mm, fixed length / random length, can be cut / chamfered / threaded

2. Tolerances (Precision Grade)

Outer Diameter: ±0.05–±0.1 mm

Wall Thickness: ±0.05–±0.1 mm

Straightness: ≤0.5 mm/m

3. Surface Finish

Pickled and bright (industrial standard), sandblasted, brushed, mirror polished, anodized (colored)

 

Products showcase of Gr5 Titanium seamless pipes

Gr5 Titanium seamless pipes
Gr5 Titanium seamless pipes for sale
Gr5 Titanium seamless pipes supplier
Gr5 Titanium seamless pipes manufacturer

contact us

 

Gr5 Titanium seamless pipes E-mail: garychen3215@hotmail.com

Gr5 Titanium seamless pipes Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

Gr5 Titanium seamless pipes Contact: Mr. Gary Chen

Gr5 Titanium seamless pipes Phone: +86-917-8883215

Gr5 Titanium seamless pipes Mobile/WhatsApp: +86 13092900605

 

Hot Tags: gr5 titanium seamless pipes, China gr5 titanium seamless pipes manufacturers, suppliers, factory, 3in titanium pipe, 4 titanium pipe, titanium 3 inch tubing, titanium tubing coil, titanium tubing for bicycles, titanium tubing for sale

Send Inquiry

(0/10)

clearall