Stainless steel is not simply "iron that doesn't rust"; rather, it features an invisible oxide film formed by chromium on the iron's surface. What, then, is the role of nickel? Nickel locks the steel into the austenite phase. Pure iron has a body-centered cubic structure (ferrite) at room temperature; it transforms into a face-centered cubic structure (austenite) when heated to 912°C and reverts upon cooling. By adding 8% to 10% nickel, the austenite phase is "frozen" at room temperature, meaning the stainless steel no longer undergoes a phase transition in its crystal structure in response to temperature changes. The properties of austenitic stainless steel-such as being non-magnetic, possessing excellent toughness, suitability for deep-drawing into thin sheets, and maintaining weld integrity without brittleness after argon arc welding-are all attributable to the face-centered cubic structure stabilized by nickel.
Kitchen-grade 304 stainless steel contains approximately 18% chromium and 8% nickel; the chromium provides corrosion resistance, while the nickel imparts toughness and ensures the chromium-based passivation layer remains intact-preventing it from flaking off-at points of bending or welding. Grade 316 stainless steel incorporates an additional 2% to 3% molybdenum specifically to withstand corrosion from seawater and chloride ions, with its nickel content raised to between 10% and 14%. Surgical instruments used in hospitals remain rust-free and retain their structural integrity after steam sterilization because their austenitic crystal structure prevents carbide precipitation at grain boundaries during repeated thermal shocks from the steam. Underlying all these properties is a fundamental condition: the steel possesses a face-centered cubic (FCC) crystal lattice, a structure stabilized by the presence of nickel.
Globally, approximately 68% of nickel goes into stainless steel production; in China, this figure is even higher-around 85%. As the world's largest producer of stainless steel, China consumes more than half of the global nickel supply. Laterite nickel ore from Indonesia and the Philippines is shipped through the Strait of Malacca to Chinese ports, where it is processed in blast and electric furnaces into nickel-iron alloy. This alloy is then refined in Argon-Oxygen Decarburization (AOD) converters to reduce carbon content from 3% to 0.02%, ultimately being cast into the steel plates used for your kitchen sinks, hot pot vessels, elevator door frames, and hospital sterilizers.
Nickel in Hydrogenation, Batteries, and the Earth's Core
Nickel reigns supreme as the industrial catalyst for hydrogenation. For over a century, Raney nickel-an ultrafine nickel framework obtained by leaching aluminum from a nickel-aluminum alloy with an alkaline solution-has dominated the catalytic hydrogenation process that transforms vegetable oils into solid shortenings and margarines. Nickel powder boasts an immense surface area, with a single gram offering tens of square meters of space where unsaturated carbon-carbon double bonds are saturated by hydrogen molecules. From the hydrogenation and desulfurization of petroleum products to the reduction of nitro groups to amino groups for dye and pesticide production, and the hydrogenation of aromatic hydrocarbons in coal tar into cycloalkanes, the answer in the "catalyst" column is almost invariably "nickel."
Together, Earth's inner and outer cores account for 35% of the planet's mass, consisting primarily of an iron-nickel alloy. The solid inner core, with a radius of approximately 1,200 kilometers, exists under pressures exceeding 300 gigapascals and temperatures above 6,000 K, conditions that compress iron and nickel atoms into a hexagonal close-packed crystal structure. The liquid outer core acts as a dynamo driven by the flow of electrically conducting iron-nickel fluid; as the fluid moves, it cuts across the weak magnetic field generated by Earth's rotation, and a self-exciting feedback mechanism amplifies this field-originally around 0.5 gauss-to an intensity strong enough to deflect the solar wind. Nickel plays a crucial role here by lowering the alloy's melting point, making it easier for the core to remain liquid at a given temperature and thereby ensuring the dynamo effect has persisted for over three to four billion years.

E-mail: garychen3215@hotmail.com
Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China
Contact: Mr. Gary Chen
Phone: +86-917-8883215
Mobile/WhatsApp: +86 13092900605