Home > Blog > Content

What are the four grades of titanium?

Nov 28, 2026

The "four grades" of titanium typically refer to the four standard grades of commercially pure titanium: Grade 1 through Grade 4.

The key difference among these four grades lies in the content of impurity elements such as oxygen and iron. The higher the oxygen content, the higher the strength; however, ductility and formability decrease accordingly.

The most critical distinguishing factor among the four grades is oxygen. Oxygen acts as an interstitial solute in titanium, significantly hindering dislocation motion and thereby increasing strength, but at the cost of reduced ductility and formability. Some data provide an intuitive order of magnitude: for every approximately 0.1 wt% increase in oxygen content, the strength of titanium increases by about 100–120 MPa.

Therefore, the sequence from Grade 1 to Grade 4 corresponds to a progression from low to high oxygen content, low to high strength, and high to low ductility.

Grade 1 is rarely used for load-bearing lead screws. Its value lies in its exceptional formability and corrosion resistance, making it suitable for deep-drawn parts, heat exchanger linings, and building roofs. Since lead screws must transmit axial forces, Grade 1's minimum strength is too low-unless it is used for extremely light-load adjustment applications in purely corrosive environments.

 

Grade 2 is the grade most commonly "misselected." It is the most widely used grade of commercial pure titanium, finding extensive application in chemical processing equipment, marine components, and general industrial fasteners. If a customer says, "I want a pure titanium lead screw that's corrosion-resistant and doesn't need to handle heavy loads," Grade 2 is a reasonable choice. However, it's important to note that its strength is far lower than that of Grade 5. In transmission applications involving significant axial loads or requiring long-term fatigue resistance, the strength limitations of pure titanium will quickly become apparent.

 

Grade 3 occupies an awkward position in lead screw selection. It is stronger than Grade 2, but the improvement is limited; it has better ductility than Grade 4, but this advantage is not particularly pronounced. In most lead screw applications, engineers either choose Grade 2 for cost and corrosion resistance or opt directly for Grade 5 alloy for strength; Grade 3's "middle-of-the-road" approach lacks sufficient appeal for transmission components.

 

Grade 4 is the "top-tier option" for pure titanium lead screws. It offers the highest strength among pure titanium grades, approaching the levels of some low-strength alloys, while retaining the corrosion resistance advantages of pure titanium. It is suitable for lead screws subjected to moderate loads and severe corrosion, where alloying elements cannot be introduced (such as in certain specialized chemical or medical applications). However, it is important to note that Grade 4 has an elongation of only about 15%, with a plasticity reserve significantly lower than that of Grade 2, which makes thread rolling and subsequent cold working considerably more difficult.

6mm Thickness Ti6Al4V Titanium Alloy Plate manufacturers 6mm Gr5 Titanium Alloy Plate suppliers

6mm Thickness Ti6Al4V Titanium Alloy Plate E-mail: garychen3215@hotmail.com

6mm Thickness Ti6Al4V Titanium Alloy Plate Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

6mm Thickness Ti6Al4V Titanium Alloy Plate Contact: Mr. Gary Chen

6mm Thickness Ti6Al4V Titanium Alloy Plate Phone: +86-917-8883215

6mm Thickness Ti6Al4V Titanium Alloy Plate Mobile/WhatsApp: +86 13092900605

 

Send Inquiry
Contact Us
    • Baoji Reliab Metal Materials Co.,Ltd
    • Mobile:+8613092900605
                     +8613092913521
    • E-mail:garychen3215@hotmail.com
                     boantj@163.com
    • Web:www.reliabmetal.com
    • Address:No.35 Middle of Baoti Road, Hi-Tech Development Zone, Baoji city, Shaanxi province China 721000