Home > Blog > Content

What are the Strength classification of titanium alloy plates?

Sep 08, 2025

Here are the Strength classification of titanium alloy plates as blow: 

 

1. Strength Classification of Titanium Alloy Plates

Low strength ‌: industrial pure titanium, corrosion-resistant structural components, chemical equipment;

Common strength: Aviation sheet parts, hydraulic pipes;

High strength: Aircraft load-bearing structural components, missile parts.

 

2. Key Performance Influencing Factors

1). Alloy composition design ‌

Aluminum ‌ : TI-6.5Al-1Mo-1V-2Zr contains 6.0% - 7.0% aluminum, significantly enhancing high-temperature strength;

Vanadium/chromium ‌ : in Ti-15V-3Al-3Cr-3Sn, 14% - 16% vanadium + 2.5% - 3.5% chromium to enhance the stability of the β phase.

2). Process control ‌

Forging process ‌ : multi-directional forging refines grains, reducing the crack rate of TC4 sheet by 40%;

Heat treatment ‌ : the strength of Grade 5 increases by 1200MPa after aging treatment.

3). Impurity control ‌

The oxygen content should be ≤0.15% and the iron content ≤0.3% to prevent the precipitation of brittle phases.

 

3. Intensity Requirements for Application Scenarios

Aerospace: High-temperature strength > 600MPa. Rocket fuel tanks, engine blades;

Marine engineering ‌ : Corrosion resistance + tensile strength ≥750MPa, ship hull, pressure-resistant shell;

Military equipment ‌ : ultra-high strength > 1300MPa, missile structural components, armor linings;

 

4. Strength and Plasticity Balance Technology

Welding performance ‌ : The strength of the TB6 welded joint reaches over 90% of the base material, and the elongation is 8% - 12%.

Rolling optimization ‌ : Grade 5 sheet adopts β -phase zone hot rolling + double annealing, with elongation increased by 12%.

 

Titanium alloy sheets factory supplier  grade 5 Titanium alloy plates supplier

 

Choose BAOJI RELIAB METAL for your titanium products needs.

 

If you are seeking for titanium materials such as titanium plates, bars, tubes, wires and titanium CNC machined parts, BAOJI RELIAB METAL is your one-stop supplier. We supplying the high quality titanium products with fast delivery, and 24-hours sales and after-sales services.

Contact us as below information:

Baoji Reliab Metal Materials Co.,Ltd

Tel: +86-917-8883215

Mobile: +8613092900605

              +8613092913521

E-mail: garychen3215@hotmail.com

              garychen20111031@gmail.com

Send Inquiry
Contact Us
    • Baoji Reliab Metal Materials Co.,Ltd