GR5 Titanium Alloy Plate Strip
video
GR5 Titanium Alloy Plate Strip

GR5 Titanium Alloy Plate Strip

Item name:GR5 titanium alloy plate strip
Material:Titanium Gr2, Titanium alloy Gr5(Ti-6Al-4V)
Thickness:0.5mm~50mm
Standard: ASTM B265
Width:5mm~500mm
Send Inquiry
Description
 

Products Description

 

 

What is GR5 titanium alloy plate strip?

?

 

GR5 titanium alloy plate strips are plate-shaped or strip-shaped materials made of titanium as the base element and other metals (such as aluminum, vanadium, etc.) added. It features light weight and high strength.

 

There are two types of allocrystalline structures of titanium alloys: it is close-packed hexagonal α titanium below 882℃ and transforms into body-centered cubic β titanium above 882℃, which determines its high-temperature resistance and mechanical properties .

 

composition of gr5 titanium alloy plate strip

 

 

Component WT% of Grade 5 Titanium

 

Al

V

C Max

Fe Max

H Max

N Max

O Max

Ti,min

5.5~6.75

3.5~4.5

0.08

0.40

0.015

0.05

0.20

90

 

Material Data of Grade 5 Titanium Alloy

 

 

Metric

English

Remarks

Physical Properties

Density

4.51g/cc

0.163 lb/in³

 

Mechanical Properties

Hardness, Brinell

334

334

Estimated from RockwellC

Hardness,Knoop

363

363

Estimated from RockwellC

Hardness, Rockwell C

36

36

 

Tensile Strength, Ultimate

950 Mpa

138000 psi

 

Tensile Strength, Yield

880 Mpa

128000 psi

 

Elongation at Break

14%

14%

 

Charpy Impact

17 J

12.5 ft-lb

V-notch

 

Brief data of gr5 titanium alloy plate strip

 

 

1) Standard: ASTM B265, ASTM F67,AMS 4911

2) Grade: Gr.1 Gr.2 Gr.3 Gr.5 Gr.7 Gr.9 Gr.12

3) Manufacturing Processes: Rolling, Forging, Annealing

4) Size: Thickness0.8mm~50.0mm*Width100mm~1500mm*Length1000mm~6000mm

5) Features: The excellent properties of Titanium Plates include high strength, low density, good mechanical properties, corrosion resistance, high stability and so on. So Titanium & Titanium Alloy Plates always be used in airplane engine components, rockets, missile and other aircraft components.

 

In addition to that, titanium and titanium alloy plates also can be used in industrial construction , sports equipment, tableware, outdoor supplies and so on. The good performances of titanium plates make it easy to be accept and are more and more familiar by public.

 

Application scenarios of gr5 titanium alloy plate strip

 

 

Titanium alloy strips, with their lightweight, high strength, corrosion resistance and biocompatibility, occupy a key position in high-end industries and emerging fields. The core application scenarios are as follows:

 

A. Aerospace field: ‌

Engine system ‌: compressor blades/turbine discs ‌ : BT9 alloy (Ti-6Al-3.5Mo-1.5Zr-0.3Si) is used for high-temperature components below 500 ° C and has better oxidation resistance than Gr5. BT20 (Ti-6Al-2Zr-1Mo-1V) is used for welding casing structures ‌

Fatigue-resistant components ‌ : fuselage frames, wing beams and other structural parts that bear complex stress, with a weight reduction effect of over 30% ‌.

Spacecraft structure ‌: Rocket fuel tanks, satellite brackets, suitable for ultra-low temperature environments (-196℃ without cracking) ‌

 

B. Chemical engineering and energy field ‌

1) chlor-alkali industry ‌

 ruthenium-titanium anode plate ‌ : core component of electrolytic cell, current efficiency up to 97%, power consumption reduced by 15%, service life over 15 years ‌.

wet chlorine cooler ‌ : Replace graphite equipment, reducing downtime by 80%‌

2) Special medium treatment ‌

tantalum-iridium-titanium anode ‌ : resistant to 98℃ concentrated sulfuric acid corrosion (with a rate of only 0.002mm/ year), used in non-ferrous metal smelting and nuclear waste treatment ‌

3) new energy equipment ‌: Hydrogen energy vehicle hydrogen storage tanks, proton exchange membrane electrolytic cells titanium plates, supporting 3D printing precision manufacturing. ‌

 

C. Marine Engineering and Ships ‌

1) Deep-sea equipment ‌: Submarine hull, deep-sea submersible components, resistant to 50 years of seawater corrosion, dive depth 80% deeper than stainless steel .

2) Marine chemicals ‌: Seawater desalination titanium tube heat exchanger, water production ratio exceeds 10:1, maintenance cycle extended to 8 years ‌.

 

D. Medical and Bioengineering ‌

1) Implant device ‌: Orthopedic joints and dental implants use β -type titanium alloys (such as Ti-Mo-Nb series), with an elastic modulus of 55-80 gpa close to that of human bone, reducing the postoperative infection rate by 60%‌.

2) Surgical tools ‌: Cardiovascular stents, antibacterial bone screws, surface roughness Ra<0.4μm to prevent microbial growth. ‌

 

Pictures of gr5 titanium alloy plate strips 

 
gr5 titanium alloy plate strip

high quality

Strictly Inspected for each part, ensure 100% qualified delivered.

customized Sizes

Can cut or make according to customer's requested size, with thickness, width and length.

product-500-500
product-500-500

Different materials

Can supply in Titanium Gr1, Gr2, Gr3, Gr5, Gr7, Gr9, Gr12.

Fast Delivery

We can cut/produce the strips at fastest delivery time, normally within 3~5 days.

FAQ(Frequently Asked Questions

 

 

FAQ

Q: Do you supply sample for Gr5 Titanium alloy plate strip? Are there any requirements for providing samples?

A: Yes, we can supply sample in a certain quantity, normally less than 0.5kg but we can negotiate for more details as per customers' demands.

FAQ

Q: 2.Does your Gr5 Titanium alloy plate strip support OEM customization?

A:  Yes we accept OEM customization.


3.  What is the MOQ on your Gr5 Titanium alloy plate strip?
A:  Normally we have no MOQ, while different qty leads to different prices.


4.Can you make our LOGO on the Gr5 Titanium alloy plate strip?
A:  Yes we can laser-marking customer's logo on the surface of the products.

Hot Tags: gr5 titanium alloy plate strip, China gr5 titanium alloy plate strip manufacturers, suppliers, factory, titanium plate, titanium flat bar stock, titanium foil, tio2 price, rainbow titanium, 1 gram titanium price

Send Inquiry

(0/10)

clearall