ASTM B160 Nickel Alloy 200 Rod
video
ASTM B160 Nickel Alloy 200 Rod

ASTM B160 Nickel Alloy 200 Rod

Item name:ASTM B160 Nickel Alloy 200 Rod
Material:Nickel 200,Nickel 201
Standard:ASTM B160
Size:Dia1.0mm-100mm
Length:<3000mm
MOQ:5KGS
Send Inquiry
Description

What is ASTM B160 Nickel Alloy 200 Rod?

 

ASTM B160 Nickel Alloy 200 Rods are round bars with nickel as the base material (usually ≥99.5%), and are classified into ordinary and low-carbon versions according to carbon content.

Pure nickel bar means a solid, long bar made of high-purity metallic nickel.
Nickel content is generally ≥99.0%, commonly US standards 201 and 200.
Appearance: silvery-white metal, rust-resistant, tough, and relatively soft.
Shape: round bars are the most common, but square and hexagonal bars also exist.

 

What are its characteristics of ASTM B160 Nickel Alloy 200 Rod?

 

Extremely alkali resistant: Almost non-corrosive in caustic soda and strong alkaline environments, making it a "alkali-resistant wonder" in the chemical industry.
Corrosion resistant: Stable in neutral and weakly corrosive environments.
Good plasticity: Easy to process, bend, and weld.
Good electrical and thermal conductivity: Commonly used in electrodes and electronic components.
Magnetic: Can be attracted by magnets at room temperature.

 

Key physical and chemical properties of ASTM B160 Nickel Alloy 200 Rod

 

  1. Basic physical parameters: Density 8.90 g/cm³; Melting point 1455℃; Thermal conductivity at room temperature approximately 90 W/(m・K); Resistivity approximately 9.6 μΩ・cm; Paramagnetic, weakly magnetic at room temperature; Moderate coefficient of linear expansion, good dimensional stability.
  2. Core advantages of corrosion resistance: Extremely strong resistance to hot concentrated alkali solutions (NaOH/KOH), making it the first choice for the alkali production industry; Stable in neutral salt, carbonate, and acetate environments; Performs well against reducing acids and organic acids; However, caution is required in strong oxidizing acids (such as concentrated nitric acid) and chlorine-containing oxidizing media; Easily forms a dense oxide film on the surface, protecting the substrate.
  3. Mechanical properties (typical values ​​in the annealed state)
Material Tensile strength Yield strength Elongation Brinell hardness
Ni 200 380–450 MPa 100–130 MPa 40%–50% About 100 HB
Ni 201 380–420 MPa 95–120 MPa Around 45%  About 95 HB

***The strength can be significantly improved after cold working (e.g., the tensile strength in the cold working state can reach 650+ MPa), while the elongation decreases; the plasticity can be restored by annealing; it has excellent low-temperature toughness and no brittle transition problem.

 

Production process and supply status of ASTM B160 Nickel Alloy 200 Rod

 

A.Supply Conditions and Specifications:

Conditions: Soft (M, fully annealed), semi-hard, hard (Y, cold-worked);

Diameter: Standard Φ3 mm~150 mm, precision fine bars up to Φ0.8 mm, large forged rounds up to Φ450 mm; Lengths are mostly 1000 mm, 2000 mm, 3000 mm, custom lengths available upon request;

Surface: Black skin (hot rolled), pickled, bright drawn (cold drawn).

B.Manufacturing process:

Electrolytic nickel plate → Vacuum induction/arc melting → Forging billet → Hot rolling/hot extrusion → Cold drawing/cold rolling finishing → Solution annealing → Non-destructive testing, precision cutting, and packaging; High-end pure nickel bars adopt electron beam/vacuum arc remelting (VAR) to further reduce impurities and segregation.

 

Typical application areas of ASTM B160 Nickel Alloy 200 Rod

 

  1. Chemicals/Chlor-alkali: Caustic soda evaporators, alkali storage tanks, electrolytic cell electrodes, pipe fittings;
  2. Electronics/Electroplating: Vacuum tubes, cathodes, electroplating anodes, battery terminals;
  3. Energy/Nuclear Power: Nuclear reactor control rod components, hydrogen fuel cell bipolar plates;
  4. Food/Pharmaceuticals: Corrosion-resistant containers, sterile pipes, pharmaceutical equipment parts;
  5. Marine/Environmental Protection: Seawater desalination equipment, water treatment corrosion-resistant components;
  6. Welding Materials: Raw materials for pure nickel welding rods/wires.

 

Picture showcase of ASTM B160 Nickel Alloy 200 Rod

 

ASTM B160 Nickel Alloy 200 Rod
ASTM B160 Nickel Alloy 200 Rod supplier
ASTM B160 Nickel Alloy 200 Rod manufacturer
ASTM B160 Nickel Alloy 200 Rod in good price

our company introduction

 

modular-1
One-stop Titanium&Nickel products Factory in China

Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel products. With high quality controlling system, our products meeting the international standard as ASTM, ASME, AMS, JIS, DIN, TOCT, our main products including bars/rods, plates/sheets, tubes, wires, forgings rings, anodes, fasteners and CNC machined parts.

For over 12 years,Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.

how to contact us

 

ASTM B160 Nickel Alloy 200 Rod E-mail: garychen3215@hotmail.com

ASTM B160 Nickel Alloy 200 Rod Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

ASTM B160 Nickel Alloy 200 Rod Contact: Mr. Gary Chen

ASTM B160 Nickel Alloy 200 Rod Phone: +86-917-8883215

ASTM B160 Nickel Alloy 200 Rod Mobile/WhatsApp: +86 13092900605

Hot Tags: astm b160 nickel alloy 200 rod, China astm b160 nickel alloy 200 rod manufacturers, suppliers, factory

Send Inquiry

(0/10)