Chemical composition of Grade 7 Titanium solid round Bar
Grade 7 Titanium solid round Bar is an industrially pure titanium + palladium-reinforced alloy with the following basic components:
Titanium (Ti): ≥99% (matrix, providing a lightweight and corrosion-resistant framework)
Palladium (Pd): 0.12%-0.25% (core strengthening element, enhancing the self-healing ability of the passive film)
Impurity control: O ≤ 0.15%, Fe ≤ 0.30%, H ≤ 0.015% (strictly controlling brittle phases)
Physical and mechanical properties of Grade 7 Titanium solid round Bar
1. Physical properties
A. Density 4.51 g/cm³, 43% lighter than steel, key to ship weight reduction
B. Coefficient of thermal expansion (20-300°C): 8.9×10⁻⁶/°C; Excellent dimensional stability at high temperatures
C. Thermal conductivity 16.4 W/(m·K); Intensive cooling is required during processing to prevent overheating
D. Melting point 1660°C; Suitable for high-temperature equipment
2. Mechanical properties
A. Tensile strength: 480-800 MPa (lower limit in annealed state, upper limit in solution state)
B. Yield strength: 380-550 MPa (design basis for chemical pressure vessels)
C. Elongation: 20%-35% (excellent ductility, suitable for cold forming)
D. Fatigue strength (10⁷ cycles): 200-250 MPa (ensures long life for aviation structural components)
E. High-temperature strength (300°C): ≥85% retention (suitable for aviation ducts/engine mounts)
Advantages of Grade 7 Titanium solid round Bar
Core advantage ---- Corrosion resistance
1) Acidic Media: Corrosion rate in 30% sulfuric acid is 0.001 mm/year, four orders of magnitude lower than 316 stainless steel (>10 mm/year).
2) Seawater Environment: Corrosion rate on a 20-year shipboard coupon is 0.0007 mm/year, with no pitting tendency.
3) High-Temperature Oxidation: A stable TiO₂+Pd-rich layer forms below 600°C, with oxidation weight gain <1 mg/cm²·h.
4) Application scenarios: hydrochloric acid reactor seals, deep-sea pipeline flanges, nuclear power plant condenser pipes
Product specifications and implementation standards
Plates: Thickness 0.4-50mm, Width ≤ 2500mm. ASTM B265
Pipes: Ø0.8-219mm × Wall Thickness 0.1-15mm. ASTM B337/338
Bars: Ø6-500mm × L ≤ 6000mm. ASTM B348
Forgings: Maximum Projected Area 2.5m². AMS 4914
Pictures showcase of Grade 7 Titanium solid round Bar
Grade 7 Titanium solid round Bar



Grade 7 Titanium solid round Bar



About our factory

Your reliable titanium/nickel products supplier in China
Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel products. With high quality controlling system, our products meeting the international standard as ASTM, ASME, AMS, JIS, DIN, TOCT, our main products including bars/rods, plates/sheets, tubes, wires, forgings rings, anodes, fasteners and CNC machined parts.
For over 11 years,Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.
how to contact us
Website: www.reliabmetal.com
Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China
Contact: Mr. Gary Chen
Phone: +86-917-8883215
Mobile/Whatsapp: +86 13092900605
E-mail: garychen3215@hotmail.com ; boantj@163.com
Hot Tags: grade 7 titanium solid round bar, China grade 7 titanium solid round bar manufacturers, suppliers, factory, titanium tig wire, 12mm titanium rod, TIG Titanium Welding Rod, titanium sleever bar, titanium steel bar, titanium barstock