Chemical Composition of Titanium alloy round bars (Gr5)
|
GRADE Elements Elements,% |
AL, max |
V, max |
Fe , max |
C , max |
N, max |
H, max |
O, max |
Other elements total,max |
|
Grade 5 |
5.5~6.75 |
3.5~4.5 |
0.40 |
0.08 |
0.05 |
0.015 |
0.20 |
0.4 |
Mechanical Property of Titanium alloy round bars (Gr5)
|
|
Tensile Strength |
Yield Strength |
Elongation,min % |
Reduction of Area,min % |
||
|
|
ksi |
Mpa |
ksi |
Mpa |
||
|
Grade 5 |
130 |
895 |
120 |
828 |
10 |
25 |
Our Advantages:
- We supply the third-party Testing Report/Certificate with the goods for each order.
- Fast delivery. (We have stocks for main sizes titanium bars and delivery time is 1-2days; For non-standard size the delivery time is 10-15days max)
- Provide personalized packaging and laser marking such as Logo and Size.
- 24-Hours online service and E-mail response.
- Shipping methods: Express, Air cargo, Ocean.
Why choose Titanium alloy Grade 5 ?
1. Excellent specific strength: The density of titanium alloys is only 60% of that of steel (about 4.5g/cm³), but the strength can reach 980-1300MPa.
The specific strength of some titanium alloys is 23.5 times higher than that of alloy steel .
2. With strong corrosion resistance: A dense oxide film forms on the surface, which can resist erosion by seawater, strong acids, strong alkali and other medias.
Its corrosion resistance is superior to that of stainless steel. Can significantly extend service life in chemical equipment and Marine engineering.
3.Bio-compatibility : No rejection reaction to human tissues, is the ideal material for artificial joints and orthopedic implants.
How was it manufactured ?

About Our Company
We Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel, Zirconium products. With high quality controlling system, our products meeting the international standard as ASTM,ASME,AMS,JIS,DIN,TOCT and other, our main products including bars/rods,plates/sheets,tubes,wires,forgings rings,anodes,fasteners and CNC machined parts.
For over 11 years,Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.
Our e-mail addresss is garychen3215@hotmail.com,Whatsapp is 8613092900605.

Relate Products Showcase--Titanium alloy round bars




Hot Tags: titanium alloy round bars, China titanium alloy round bars manufacturers, suppliers, factory, titanium machining, titanium welding rod suppliers, titanium round bar suppliers, titanium bar suppliers, titanium bars for sale, titanium mineral