Hexagon socket head screws,also known as hexagon socket bolts,cup head screws,and hexagon socket screws for short.
Material can be made in CP titanium Gr2 Gr3, titanium alloys Ti-6Al-4V,Ti-Pd, Ti-3Al-2.5V
Surface:Can make PVD gold,black; Anodizing blue,green,purple,etc.
Send Inquiry
Description

1. Structural features

 

A. Cylindrical head hexagon socket design: It adopts a hexagonal groove structure and is compatible with standard hexagon socket wrench installation tools

B. Fine thread rod section: Compared with coarse thread, it increases the number of meshing times, enhancing the connection tightness and anti-loosening performance

C. The nominal diameter range of the applicable thread is 8mm to 36mm

 

2.  Application field

 

It is applicable to scenarios in the field of mechanical manufacturing that require high-precision connections, including

Thin-walled material fastening: Fine-threaded threads can reduce the risk of stripped threads in thin-walled materials

Precision instrument assembly: Higher thread meshing quantity enhances connection stability

Anti-loosening connection requirement: Anti-loosening effect is achieved by increasing the number of thread meshing times through a fine-thread structure

 

3. Description of Cylindrical head hexagon socket titanium screw

 

Grades: GR1, GR2, GR5, Gr7, Gr9

Features: With low specific gravity, strong corrosion resistance.

Standard: DIN933, DIN931, DIN963, DIN84, GB/T5780, DIN912, DIN7380, DINEN1665, DIN7991, DIAN934, DIAN126, DIN127, British BSW, American UNC, Drawing processing

Bolts types: Hexagonal Bolt, Inner Hexagonal Bolt, Countersunk inner hexagonal bolt, Countersunk cross Bolt, conical Head Bolt, countersunk straight Head Bolt, Hexagonal flange face Bolt, Cylindrical Head bolt, Hexagonal Nut, Flat Washer, Spring Washer.

 

Besides, according to customer requirements, we can undertake the production of titanium processed parts, titanium alloy machined parts, titanium standard parts, titanium non-standard parts, as well as processing based on provided drawings and materials.

 

Processing applications: Chemical equipment, medical accessories, home appliance accessories, photographic equipment, auto and motorcycle parts, electronics factories, powder metallurgy, optoelectronic technology, furniture accessories, food machinery, and various other non-standard precision CNC turning processing products.

 

4. Pictures of Cylindrical head hexagon socket titanium screw

 

Cylindrical Head Hexagon Socket Titanium Screw
Socket head titanium alloy bolts
Cylindrical Head Hexagon Socket Titanium Screw supplier
Sizes of Titanium Inner Hexagonal Bolts

 

PVD Black Cylindrical Head Hexagon Socket Titanium Screw
PVD Black titanium alloy screws
High quality Cylindrical Head Hexagon Socket Titanium Screw
Half threading titanium bolts

5. product Mechanical Property chart

 

Grade

Tensile Strength,min

Yield Strength,min

Elongation,%

Ksi

MPa

Ksi

MPa

Gr 1

35

240

20

138

24

Gr 2

50

345

40

275

20

Gr 3

65

450

55

380

18

Gr 4

80

550

70

483

15

Gr 5

130

895

120

828

10

Gr7

50

345

40

275

20

Gr 9

90

620

70

483

15

Gr 12

70

483

50

345

18

Gr 23

120

828

110

759

10

 

 

Hot Tags: cylindrical head hexagon socket titanium screw, China cylindrical head hexagon socket titanium screw manufacturers, suppliers, factory, titanium fasteners usa, titanium alloy fasteners, titanium socket head cap screws, titanium shoulder bolts, anodized titanium bolts, titanium screws for sale