Products definition
Titanium Spring Washers DIN127, also known as titanium spring washers or titanium open-ended spring washers, are ring-shaped elastic fasteners with a beveled cut that generate sustained axial tension through elastic deformation, effectively preventing bolts from loosening under vibration, impact, or temperature cycling conditions. Precision-manufactured from aerospace-grade titanium alloy (GR2 / GR5 Ti-6Al-4V), they combine four core advantages-**ultra-lightweight, high corrosion resistance, high specific strength, and non-magnetic properties**-making them an ideal upgrade and replacement for steel and stainless steel spring washers.
common Materials
GR2 (Industrial-Grade Pure Titanium)
- Tensile strength ≥345 MPa, yield strength ≥275 MPa
- Good formability and excellent corrosion resistance
- Suitable for: general corrosive environments, lightweight applications, and routine marine/chemical service conditions
GR5 (Ti-6Al-4V Titanium Alloy)
- Tensile strength ≥895 MPa, yield strength ≥828 MPa
- High strength, high elasticity, fatigue resistance, and superior heat resistance
- Suitable for: Severe operating conditions involving intense vibration, heavy loads, and high temperatures (aerospace, motorsports, wind power, etc.)
Technical Specifications Table
| Specs | ID d (mm) | OD D (mm) | THKs (mm) | Height H (mm) | Unit weight (g/GR5) |
|---|---|---|---|---|---|
| M2 | 2.1 | 4.4 | 0.5 | 1.0 | 0.08 |
| M3 | 3.1 | 6.2 | 0.8 | 1.5 | 0.18 |
| M4 | 4.1 | 7.6 | 0.9 | 2.0 | 0.32 |
| M5 | 5.1 | 9.2 | 1.0 | 2.5 | 0.50 |
| M6 | 6.2 | 11.0 | 1.2 | 3.0 | 0.80 |
| M8 | 8.2 | 14.0 | 1.5 | 4.0 | 1.60 |
| M10 | 10.2 | 17.0 | 1.8 | 5.0 | 2.80 |
| M12 | 12.3 | 19.0 | 2.0 | 6.0 | 4.20 |
| M16 | 16.3 | 24.0 | 2.5 | 8.0 | 8.50 |
| M20 | 20.5 | 30.0 | 3.0 | 10.0 | 15.0 |
Standards & Specifications
Standards: DIN 127B / ISO 127 (Standard Spring Washers)
Type: Standard Open-Ended Beveled (Single Coil Spring Washer)
Common Sizes (Matching Threads): M3 / M4 / M5 / M6 / M8 / M10 / M12 / M14 / M16 / M20
Compatibility: Used in sets with corresponding titanium screws and titanium nuts
Core Advantages
1. Extreme Lightweight Design
Titanium alloy has a density of approximately 4.43–4.51 g/cm³, making it about 40% lighter than ordinary steel gaskets and only about 60% as dense as stainless steel. In weight-sensitive fields such as aerospace, motorsports, and lightweight robotics, this advantage directly reduces structural loads and energy consumption.
2. Absolute Corrosion Resistance
Unlike galvanized steel washers or even stainless steel washers, titanium is completely inert to seawater, chloride ions, industrial chemicals, and acids; it will not rust or degrade. In harsh corrosive environments such as marine engineering, desalination, and chemical piping, titanium alloy spring washers can maintain joint integrity over the long term.
3. High Strength and Excellent Elasticity
GR5 (Ti-6Al-4V) titanium alloy has a tensile strength of over 895 MPa and a yield strength of ≥828 MPa, providing spring force and hardness comparable to high-strength steel lock washers, yet weighing only about 45% as much. Pure titanium GR2 spring washers retain more than 85% of their initial spring force even after repeated compression.
4. Non-magnetic
Titanium is a non-ferromagnetic material that does not interfere with the normal operation of precision electronic instruments, semiconductor manufacturing equipment, medical devices (such as MRI machines), or high-energy physics equipment.
5. Stability Across a Wide Temperature Range
GR2 spring washers are suitable for temperatures ranging from -252°C to 315°C, while GR5 spring washers can withstand temperatures from -252°C to 538°C, maintaining stable elasticity in both extremely high and low-temperature environments.
6. Aesthetic Surface Treatment Options
Titanium alloys naturally possess excellent surface coloring capabilities. Through anodizing, they can be finished in a variety of colors, including gold, blue, and purple, combining functionality with visual appeal. They are suitable for applications such as high-end consumer electronics and custom bicycle/motorcycle modifications.
Applications
*** Aerospace
Aircraft structural components, engine accessories, lightweight satellite connections - Weight reduction means extended range; highly reliable and maintenance-free.
*** Medical Devices
Surgical instruments, rehabilitation equipment, orthopedic implants, MRI-compatible devices - Non-magnetic, biocompatible, and resistant to corrosion from bodily fluids.
*** Offshore Engineering
Marine hardware, offshore platforms, desalination equipment, submarine components - Resistant to seawater and chloride ion corrosion, with a service life far exceeding that of stainless steel.
*** New Energy
Wind turbine towers, solar mounting systems, hydrogen energy equipment, battery pack connections - Excellent weather resistance, lightweight design for cost reduction.
*** Chemical and Petroleum Industries
Pipe flanges, valves, reactors, pump housings - Resistant to corrosion from acids, alkalis, and chemical media.
*** Automotive / Racing / Motorcycle Modifications
Chassis, suspension, rims, lightweight engine modification parts - Reduces weight, resists vibration, resists corrosion, and enhances performance.
*** Bicycles / Outdoor Sports
Road bike / mountain bike frames, handlebar stems, seatposts, disc brakes, derailleurs, pedals - Weight reduction, rust prevention, resistance to pedaling vibrations, and more attractive color options through anodizing.
*** Drones / Model Aircraft / Robots
Frames, arms, gimbals, motors, flight controller mounts - lightweight for extended flight time, non-magnetic to prevent sensor interference, and vibration-resistant for stable flight.
*** Precision Instruments / Electronics / 3C
Test equipment, communication base stations, radar, high-end consumer electronics - non-magnetic to prevent interference, precision assembly.
Products display






surface treatment
**Natural Finish**: Natural titanium color with a silver-gray metallic texture; standard option
**Electrolytic Polishing**: Surface roughness Ra ≤ 0.8 μm; brighter finish with further enhanced corrosion resistance
**Passivation**: Reinforces the surface passivation film; suitable for extreme corrosive environments
**Anodizing** Available in gold, blue, black, rainbow, and other colors; serves both decorative and identification purposes without affecting dimensional accuracy
contact us
E-mail: garychen3215@hotmail.com
Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China
Contact: Mr. Gary Chen
Phone: +86-917-8883215
Mobile/WhatsApp: +86 13092900605
Hot Tags: titanium spring washers din127, China titanium spring washers din127 manufacturers, suppliers, factory, blue titanium bolts, cheap titanium bolts, titanium button head screws, titanium clevis pin, titanium socket head screw, titanium threaded rod