ASTM B861 Titanium Seamless Tube For Aircraft Industry
video
ASTM B861 Titanium Seamless Tube For Aircraft Industry

ASTM B861 Titanium Seamless Tube For Aircraft Industry

ASTM B861 Titanium Seamless Tube for Aircraft Industry
Material:Grade 2,Grade 3,Grade 5(Ti-6Al-4V),Grade 9(Ti-3Al-2.5V),Grade 12
Type: Seamless tube/pipe
Form:Round shape
Specification:OD5mm-150mm*WT0.5mm-15mm
Length:Less than 6000mm,can cut into customer length
Send Inquiry
Description
1

Products introduction

 

ASTM B861 Titanium Seamless Tubes for Aircraft Industry are tubes made from titanium or titanium alloys that are formed through piercing or hot extrusion, followed by cold rolling or cold drawing, and feature no weld seams. Their core value lies in their "high specific strength + excellent corrosion resistance + absence of weld-related risks," but this comes at the cost of high prices, stringent processing and welding requirements, low elastic modulus, and greater susceptibility to hydrogen damage and contamination.

ASTM B861, "Standard Specification for Titanium and Titanium Alloy Seamless Pipe," is the most widely applied and frequently cited general product standard in the global titanium seamless pipe industry. B861 itself is a general industrial standard for "general corrosion resistance and high-temperature service" and is not a standard specific to the aerospace industry-aerospace engineering procurement typically uses it as a foundation and then overlays it with AMS/MIL aerospace-specific standards (see Section 9 for details). This standard has been approved by the U.S. Department of Defense for defense procurement.

 

2

Common Grades and Correspondences

 

International Designations Features Typical Applications
Gr1 / Gr2 / Gr3 Industrial-grade pure titanium offers excellent corrosion resistance and weldability, with strength increasing as the grade rises. Chemical, Seawater, Heat Exchanger Tubes, General-Purpose Pressure Tubes
Ti-0.2Pd, Gr7 Adding Pd improves resistance to reducing acids and crevice corrosion Contains chloride ions, weak reducing acids, and relatively harsh media
Ti-0.3Mo-0.8Ni, Gr12 It is more resistant to reducing environments such as hydrochloric acid and sulfuric acid than pure titanium, and has slightly higher strength. Chemical processing applications involving high chlorine levels and reducing acids
Ti-6Al-4V,Gr5 High strength; less corrosion-resistant and less stable than pure titanium; higher cost and more difficult to machine Aviation hydraulics, high-strength structures, and certain medical applications

 

3

Key Performance Characteristics

 

1. Density is approximately 4.5 g/cm³, about 60% that of steel; it has outstanding specific strength.
2. The modulus of elasticity is approximately 110 GPa, about half that of steel; it has low stiffness and high springback, so the spacing of pipe system supports and thermal expansion compensation must be recalculated.
3. The melting point is approximately 1668°C; however, the long-term oxidation resistance of industrial-grade pure titanium should not be interpreted solely based on its "high melting point." Conventional designs typically limit operating temperatures to below approximately 425°C; the decline in high-temperature strength and the thickening of the oxide film must be evaluated separately.
4. Corrosion resistance depends on a dense TiO₂ passivation film: it performs very well in seawater, wet chlorine, chlorides, nitric acid, chromic acid, and most oxidizing media.
5. Weaknesses: Crevice corrosion may occur in hot, concentrated chloride solutions; pure titanium is unstable in reducing acids such as hydrochloric acid and sulfuric acid; hydrofluoric acid and fluorinated media cause severe corrosion; hydrogen absorption can lead to hydrogen embrittlement, so caution is required regarding over-cathodic protection, improper acid washing, and high hydrogen partial pressure at elevated temperatures.
6. Compared to stainless steel: It is lighter and more resistant to seawater and chloride pitting and crevice corrosion, but it has relatively low thermal conductivity, low stiffness, is more expensive, and requires high manufacturing cleanliness standards.

 

4

Chemical Composition (ASTM B861, wt%)

 

Elements Gr.1 Gr.2 Gr.3 Gr.9 (Ti-3Al-2.5V) Gr.23 (Ti-6Al-4V ELI) Gr.5 (Ti-6Al-4V)
N max 0.03 0.03 0.05 0.03 0.03 0.05
C max 0.08 0.08 0.08 0.08 0.08 0.08
H max 0.015 0.015 0.015 0.015 0.0125 0.015
Fe max 0.20 0.30 0.30 0.25 0.25 0.40
O max 0.18 0.25 0.35 0.15 0.13 0.20
Al - - - 2.5-3.5 5.5-6.5 5.5-6.75
V - - - 2.0-3.0 3.5-4.5 3.5-4.5
Other Elements (Individual / Total) 0.1 / 0.4 0.1 / 0.4 0.1 / 0.4 0.1 / 0.4 0.1 / 0.4 0.1 / 0.4

 

5

Mechanical Properties at Room Temperature (ASTM B861, Minimum Values)

ASTM B861 Titanium Seamless Tube for Aircraft Industry

6

Typical Applications

 

Chemical Industry Heat Exchangers/Condensers: GR1/GR2 are preferred for seawater, brine, and chloride-containing media; select GR7/GR12 if there is a risk of crevice corrosion or exposure to weakly reducing acids.

Petrochemical, chlor-alkali, wet chlorine, and oxidizing acids: Pure titanium is often suitable, but temperature, concentration, pH, crevice formation, and flow velocity must be verified.

High-pressure or aerospace hydraulic applications: GR5 can reduce weight and improve strength, but it imposes stricter requirements regarding fatigue, stress corrosion, the heat-affected zone of welds, and non-destructive testing.

 

7

Products Dis

ASTM B861 Titanium Seamless Tube for Aircraft Industry
ASTM B861 Titanium Seamless Tube for Aircraft Industry supplier
ASTM B861 Titanium Seamless Tube for Aircraft Industry manufacturer
ASTM B861 Titanium Seamless Tube for Aircraft Industry in stocks
8

testing equipments

 

who we are?

One-stop Titanium Processing Parts Factory in China

We Baoji Reliab Metal Material Co.,Ltd was founded in year 2014, located in the famous 'China Titanium Valley--BAOJI', under the strong R&D ability and continuously development, our mainly products have including titanium&titanium alloy bars/rods, plates, tubes, forgings, fasteners&machined parts, also zirconium and nickel products.

We have passed the Quality System Certificate of ISO 9001-2015, aiming for the satisfactions of different customers' requests.

high quality

Advanced Equipment

Professional Team

One-Stop Solution

ASTM B861 Titanium Seamless Tube for Aircraft Industry

Testing and Inspection Laboratory

ASTM B861 Titanium Seamless Tube for Aircraft Industry

Hardness Tester

ASTM B861 Titanium Seamless Tube for Aircraft Industry

Universal Mechanical Testing Machine

ASTM B861 Titanium Seamless Tube for Aircraft Industry

Arc Spark Direct-Reading Spectrometer

9

FAQ

 

Q: What size of the Titanium tubes that you can supply?

A:We can supply titanium tubes diameters from 5.0mm to 150mm, and can produce according to customers specs.

 

Q: Do you provide a material certificate?

A: Yes, every batch ships with a mill test certificate covering chemical composition and mechanical properties.

 

Q: Can the ASTM B861 Titanium Seamless Tube for Aircraft Industry be cut to my length?

A: Yes, precision cut-to-length is available before shipment.

 

Q: What is the MOQ?

A: Our MOQ is 5kgs.

 

10

contact us

 

ASTM B861 Titanium Seamless Tube for Aircraft Industry E-mail: garychen3215@hotmail.com

ASTM B861 Titanium Seamless Tube for Aircraft Industry Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

ASTM B861 Titanium Seamless Tube for Aircraft Industry Contact: Mr. Gary Chen

ASTM B861 Titanium Seamless Tube for Aircraft Industry Phone: +86-917-8883215

ASTM B861 Titanium Seamless Tube for Aircraft Industry Mobile/WhatsApp: +86 13092900605

 

Hot Tags: astm b861 titanium seamless tube for aircraft industry, China astm b861 titanium seamless tube for aircraft industry manufacturers, suppliers, factory, 1 titanium tubing, 4 titanium pipe, small diameter titanium tubing, ti titanium, titanium chains, titanium price per kg

Send Inquiry

(0/10)

clearall