Item name:Gr5 titanium alloy square tube
Material:Titanium Gr1, Gr2, Gr3, Gr4;Titanium alloy Grade 5 Ti-6Al-4V
Producing type:Forged and Rolled
MOQ:1 piece
Send Inquiry
Description

What is Gr5 titanium alloy square tube?

Titanium square tubes have a wide range of applications in many fields due to their excellent properties, such as high strength, low density, good corrosion resistance, and ability to withstand extreme temperatures. Gr5 titanium alloy square tube can be used to form various load-bearing components according to different structural requirements and can also serve as connectors between components.

 

With a density of 4.5 g/cm³, it is 45% lighter than stainless steel but boasts a strength of 1100 MPa. Its corrosion resistance lifespan is three times that of ordinary materials, and it is suitable for environments with a pH value of 1-13. The operating temperature range is -196℃ to 600℃.

 

Products Features of Gr5 titanium alloy square tube

1.Good plasticity

2.Excellent forming performance

3.Easy to weld

4. High temperature working temperature can reach 300℃

5. High strength

6.Good corrosion resistance

7. High heat resistance

* Mainly used as corrosion-resistant structural material, with good corrosion resistance, oxidation resistance is better than most austenitic stainless steel; but the heat resistance is poor, the use temperature should not be too high.

* Widely used in various equipment structures and engineering structures, such as transmission towers, lifting and transportation machinery, ships, industrial furnaces, reaction towers, container racks and warehouse shelves, etc.

 

Applicaitons of Gr5 titanium alloy square tube

Gr5 titanium alloy square tube are widely used in a variety of fields due to their excellent properties, such as high strength, low density, good corrosion resistance, and ability to withstand extreme temperatures.

 

The following are some of the main applications:

1. Aerospace: Titanium extrusions are used in aircraft and spacecraft to manufacture structural components such as wing spars, landing gear, and engine components, as they require lightweight yet strong materials to improve fuel efficiency and support high performance requirements.

2. Chemical Industry: In the chemical processing industry, titanium extrusions are used to manufacture reaction vessels, heat exchangers, and other equipment exposed to corrosive media, taking advantage of their excellent corrosion resistance.

3. Medical Industry: Titanium extrusions are also used in the biomedical field, such as in the manufacture of artificial joints, dental implants, and medical devices, due to titanium's biocompatibility and non-toxic properties.

4. Marine Engineering: In shipbuilding and offshore platforms, titanium extrusions can be used to construct parts that come into contact with seawater, such as propeller shafts, pump bodies, and piping systems, to resist seawater corrosion.

5. Automotive Manufacturing: Despite their high cost, titanium extrusions are also used in key components such as exhaust systems, connecting rods, and springs in racing cars and high-end vehicles, driven by the pursuit of high performance and weight reduction.

6. Sports Equipment: High-end sporting goods such as golf clubs and bicycle frames also utilize titanium extrusions to provide a better strength-to-weight ratio and durability.

7. Building and Structural Applications: Titanium extrusions may be used in certain special architectural structures, particularly those designed to withstand harsh environmental conditions, such as near seaside locations or in heavily polluted areas.

8. Energy Industry: Power generation facilities, including nuclear power plants, sometimes use titanium extrusions as cooling system components due to its excellent resistance to many coolants.

 

Available sizes of Gr5 titanium alloy square tube

 

A. 20*20*1 20*20*1.5 20*20*2mm

B. 25*25*1 25*25*2 25*25*3mm

C. 30*30*1.5 30*30*2 30*30*2.5 30*30*3mm

D. 40*40*1 40*40*2 40*40*2.3 40*40*3 40*40*4 40*40*5 40*40*6mm

E. 50*50*1.5 50*50*2 50*50*3 50*50*4mm

F. 60*60*1.5 60*60*2 60*60*3 60*60*4 60*60*5 60*60*6mm

G. 80*80*3 80*80*4 80*80*5 80*80*6 80*80*8mm

 

Products Showcase of Gr5 titanium alloy square tube

Titanium square tube
Polished titanium alloy square tube
Ti-6AL-4V titanium square tubing in stocks
Grade 5 titanium square pipe for sale

Company introduction

 

We Baoji Reliab Metal Material Co.,Ltd was founded in year 2013, located in the famous 'China Titanium Valley--BAOJI', under the strong R&D ability and continuously development, our mainly products have including titanium&titanium alloy bars/rods, plates, tubes, forgings, fasteners&machined parts, also zirconium and nickel products. We have passed the Quality System Certificate of ISO 9001-2015, aiming for the satisfactions of different customers' requests.

 

contact us 

Gr5 Titanium Alloy Square Tube E-mail: garychen3215@hotmail.com ; boantj@163.com

Gr5 Titanium Alloy Square Tube Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

Gr5 Titanium Alloy Square Tube Contact: Mr. Gary Chan/Ms. Sophia

Gr5 Titanium Alloy Square Tube supplier Phone: +86-917-8883215

Gr5 Titanium Alloy Square Tube for sale Mobile/WhatsApp: +86 13092900605

Hot Tags: gr5 titanium alloy square tube, China gr5 titanium alloy square tube manufacturers, suppliers, factory, titanium tubing for bike frames, titanium dioxide price, 4 titanium tubing, 3 inch titanium pipe, titanium tubing cost, ti 3al 2 5 v tubing

Send Inquiry
Contact Us
    • Baoji Reliab Metal Materials Co.,Ltd


(0/10)

clearall