Shaanxi Province, as the core area of China's titanium industry, produced and processed nearly 70,000 tons of titanium materials in 2024, with an annual output value exceeding 60 billion yuan, accounting for 65% of the national output and 33% of the global output, making it the world's largest producer. Baoji City, known as "China's Titanium Valley," is home to leading enterprises such as Baoji Titanium Group, forming a complete industrial chain from sponge titanium raw materials to finished products. Its products are widely used in major national projects such as aerospace and deep-sea exploration.
A. Technological Innovation and Breakthroughs
1.High-End Manufacturing Technology
Baoji Titanium Group has overcome key technologies such as the development of wide-width thick titanium alloy plates and the integral forming of titanium alloy hemispheres. Its developed manned cabin spherical shell model has been applied to deep-sea submersibles, filling a domestic technological gap.
China's first hot continuous rolling production line for titanium and titanium alloys has been put into operation, capable of rolling 150 mm diameter billets into 0.8 mm wire coils in a single pass, improving material supply capabilities in aerospace, medical devices, and other fields.
2.Medical Applications
Due to its density being close to that of human bone and its excellent biocompatibility, titanium alloys have been widely used in implants such as femoral stems and bone plates, essentially replacing traditional stainless steel products. New medical titanium alloys, such as Ti-6Al-7Nb, have further reduced health risks through optimized formulations.
B. Expanding Emerging Application Scenarios
1.Consumer Electronics
Titanium alloys are entering the mobile phone frame market. Apple's iPhone 15 Pro series uses titanium alloy frames, achieving a balance between strength and weight. Xiaomi launched a special titanium edition, using aerospace-grade high-purity titanium and aluminum alloy composites to enhance durability.
There are now over 200 types of consumer titanium products, including foldable screen phone body materials and titanium screws. BaoTi Group is collaborating with leading companies to accelerate product diversification.
2.Humanoid Robots
Due to its lightweight and high-strength properties, titanium alloys have become ideal materials for biomimetic joints and load-bearing skeletons. Tesla's Optimus Gen3's titanium alloy gear set reduces joint weight by 40% and increases fatigue life by 3 times. Medical-grade titanium alloys developed by domestic companies have passed robot cycle testing.
Driven by policy, domestic orders for titanium alloys for robots surged by 217% year-on-year in the first quarter of 2025, with monthly production capacity exceeding 80 tons.
The China Titanium Valley International Titanium Industry Expo has been held annually in Baoji since 2015, becoming an important platform for global titanium industry technology exchange and achievement display. It attracts upstream and downstream enterprises and service providers to participate, promoting industrial upgrading.
Titanium alloys are transitioning from "national strategic equipment" to everyday life, with their innovative applications continuously expanding, signifying a strong momentum for materials science towards high-end and diversified development.

Baoji Reliab Metal Materials Co.,Ltd
Mobile: 0086 13092900605
Sales Department 1: WhatsApp +8613092900605 (Mr.Gary)
Sales Department 2: +8613092913521(Ms. Sophia)
Address: No.35 Baoti Rd, Weibin District, Baoji, China