Small Diameter Titanium Rod For Medical
video
Small Diameter Titanium Rod For Medical

Small Diameter Titanium Rod For Medical

Product name:Small Diameter Titanium Rod For Medical
Standard:ASTM F67,ASTM F136,ISO 5832-2,ISO 5832-3
Size:Dia1.0mm-25mm;Length <3000mm
MOQ: 1kg
Send Inquiry
Description
1

Introduction of Small Diameter Titanium Rod For Medical

 

Small Diameter Titanium Rod For Medical refer to medical-grade titanium and titanium alloy rods with a diameter of ≤25mm. They primarily adhere to the international standard ISO 5832 and are characterized by high precision, high biocompatibility, and ease of shaping and processing. They serve as the core base material for miniature implants in fields such as dentistry, minimally invasive orthopedics, and neurosurgery.

It possesses excellent biocompatibility, mechanical adaptability, and resistance to body fluid corrosion, making it a core base material for implantable devices in orthopedics, dentistry, neurosurgery, and other fields.

The core value of Small Diameter Titanium Rod For Medical lies in their compatibility with the human physiological environment, requiring them to simultaneously meet three key requirements: biocompatibility, mechanical matching, and processability.

 

2

Main grades and key parameters of Small Diameter Titanium Rod For Medical

 

  • GR1ELI: φ0.5~25mm, Ti ≥ 99.85%, O ≤ 0.12%, ultra-low interstitial elements, Tensile strength ≥ 345 MPa,Yield strength ≥ 240 MPa,Elongation ≥ 25%,Hardness HV 120-150, It has excellent plasticity, is easy to bend and weave, and is non-allergenic.
  • GR2ELI: φ1~20mm, Ti ≥ 99.75%, O ≤ 0.16%, offering the best value for money. Tensile strength ≥ 415 MPa,Yield strength ≥ 275 MPa,Elongation ≥ 20%,Hardness HV 130-170; It offers a balance of strength and ductility, along with optimal biocompatibility.
  • TI6AL4VELI:φ1.0~30mm, Ti-6Al-4V ELI, O≤0.13%, no harmful ion precipitation.Tensile strength ≥ 860 MPa, yield strength ≥ 795 MPa, elongation ≥ 10%, hardness HV 280-350. High strength and fatigue resistance, suitable for minimally invasive load-bearing fixation.

 

3

Key performance requirements for Small Diameter Titanium Rod For Medical (medical implant rigid specifications)

 

1. Biocompatibility

Cytotoxicity: ≤ Grade 1 (ISO 10993-5), no apoptosis;

Sensitization/Irritation: No sensitization reaction, skin irritation score 0;

Hemolysis rate: ≤5% (ISO 10993-4), no risk of hemolysis.

2. Dimensions and Surface Accuracy

Diameter tolerance: ±0.001mm for φ≤3mm, ±0.002mm for φ3~10mm;

Surface quality: No scratches, pits, or grinding burns under 10x magnification, no residual grinding debris;

No residual stress: Low-temperature stress relief annealing (150℃×1h) to prevent deformation caused by stress release after implantation.

3. Resistance to Body Fluid Corrosion

Simulated body fluid immersion test (37℃ Hank's solution, 72h), corrosion rate ≤0.0005mm/year, no pitting or rusting on the surface, no metal ion precipitation.

 

4

Typical application scenarios for Small Diameter Titanium Rod For Medical

 

1. Dentistry
Dental implants: GR2ELI φ3~6mm, sandblasted and acid-etched surface (Ra1.5-3μm), promoting bone tissue ingrowth;
Orthodontic wires/brackets: GR1ELI φ0.5~1mm, good plasticity, can be bent into complex shapes, non-magnetic and does not affect CT scans.
2. Minimally Invasive Orthopedics
Phalangeal/metacarpal fixation pins: GR2ELI φ1~3mm, suitable for minimally invasive surgery, easy to implant and good biocompatibility;
Spinal minimally invasive fixation rods: TI6AL4VELI φ5~10mm, high strength and fatigue resistance, suitable for intervertebral body fixation.
3. Neurosurgery
Cranial miniature fixation pins: GR2ELI φ1~2mm, non-magnetic, does not affect magnetic resonance imaging (MRI) examinations, avoiding interference with postoperative diagnosis.
4. Other Fields
Cardiovascular stent substrate: GR1ELI φ0.5~1mm, thin-walled rod, can be laser cut into a mesh stent;
Cochlear implant electrodes: GR2ELI φ0.3~0.5mm, good conductivity and resistance to body fluid corrosion.

 

5

Products Pictures of Small Diameter Titanium Rod For Medical

 

Small Diameter Titanium Rod For Medical
Small Diameter Titanium Rod For Medical supplier
Small Diameter Titanium Rod For Medical manufacturer
High Quality Small Diameter Titanium Rod For Medical
6

Company introduction

 

Small Diameter Titanium Rod For Medical
TO BE YOUR RELIABLE AND TRUSTABLE PARTNER AS ALWAYS!

Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel,Zirconium products. With high quality controlling system, our products meeting the international standard as ASTM, ASME, AMS, JIS, DIN, TOCT, our main products including bars/rods, plates/sheets, tubes, wires, forgings rings, anodes, fasteners and CNC machined parts.

For over 11 years,Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.

 

7

how to contact us

 

Small Diameter Titanium Rod For Medical E-mail: garychen3215@hotmail.com

Small Diameter Titanium Rod For Medical Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China

Small Diameter Titanium Rod For Medical Contact: Mr. Gary Chen

Small Diameter Titanium Rod For Medical Phone: +86-917-8883215

Small Diameter Titanium Rod For Medical Mobile/WhatsApp: +86 13092900605

 

Hot Tags: small diameter titanium rod for medical, China small diameter titanium rod for medical manufacturers, suppliers, factory, titanium sleever bar, titanium rectangular bar, titanium tig wire, titanium s, titanium mineral, titanium rod suppliers