Ti-3AI-2.5V Alloy Rod and Bar
video
Ti-3AI-2.5V Alloy Rod and Bar

Ti-3AI-2.5V Alloy Rod and Bar

Brand Name:RLD
Application:Sports, Outdoor Accessories, Fasteners, Semiconductor, Petroleum
Shape:Round, Square
Diameter: Dia3.0mm~dia150mm
Length:10~6000mm
Standard:ASTM B348 AMS4928 AMS 4911 ASTM F136 ISO 5832-3
Certificate: ISO 9001: 2015 EN 1024 3.1 EN 1024 3.2
Surface:Polishing,Grinding
Send Inquiry
Description

The definition of Titanium alloy rod and bar

 

Ti-3AI-2.5V alloy rod and bar are one of the excellent metallic titanium bars.

 

Titanium is a versatile and lightweight metal known for its exceptional strength, corrosion resistance, and bio-compatibility. It has a high strength-to-weight ratio, making it ideal for applications where both strength and low weight are critical. Titanium exhibits excellent resistance to corrosion, including in harsh environments such as seawater and acidic conditions. Additionally, its bio-compatibility makes it suitable for medical implants and surgical instruments.

 

We understand the importance of quality and reliability in titanium products. Therefore, we source our materials from reputable manufacturers who adhere to stringent quality control standards. All our titanium products undergo thorough testing to ensure they meet industry standards and exceed customer expectations.

 

Specification of titanium alloy rods and bars

 

Product Name

Ti-3AI-2.5V alloy rod and bar

Material

Gr1,Gr2,Gr3,Gr4,Gr5(Ti-6Al-4V),Gr7,Gr9,Gr11,Gr12,Gr23(Ti-6Al-4V Eli),Gr28

Standard

ASTM B348, F67, F136, AMS4928,AMS4967,AMS4931

Specification

Round bar: Dia(6-300mm) *Length or as customized

Hex bar : SW(4-100mm)*Length or as customized
Squarer bar: W(6-100mm)*TK(6-100)*Length

Surface

Polished,machined,peeled

Product Type

Round, Square, hexagonal

Certification

AS9100D,NORSOK M650 PED 4.3

Technique

Hot rolled or cold rolled

Application

Chemical industry
Petrochemical industry
Machining field,Automobile field,etc.
Textile printing and dyeing
industry, and so on.

Quality and Test

Test and inspections ensure the materials meet destructive and non-destructive test according to industry and customers specifications.

 

Mechanical Property of titanium round bars

 

Mechanical properties

Grade

Condition

Tensile Strength (Rm/Mpa) ≥

Yield Strength (Rp0.2/Mpa)

≥

Elongation (A%)

≥

Reduction of Area (Z%)

≥

Ti-6Al-4V ELI

M

860

795

10

25

Grade 5 (Ti-6Al-4V)

M

860

780

10

/

Grade9 (Ti-3AL-2.5V)

M

620

483

15

25

 

Ten Properties of Titanium

 

  1. Low Density, High specific strength
  2. Excellent corrosion resistance
  3. Good heat resistance
  4. Good Low temperature performance
  5. Strong Anti damping performance
  6. Non-magnetic, Non-toxic
  7. Small heat conduction coefficient
  8. Low modules of elasticity
  9. The suction performance
  10. Tensile strength close to the yield strength

 

FAQ(Frequently Asked Questions)

 

Q: Do you supply sample for Ti-3AI-2.5V alloy rod and bar? Are there any requirements for providing samples?

A: Yes, we can supply sample in a certain quantity, normally less than 0.5kg but we can negotiate for more details as per customers' demands.

Q: Do you make Ti-3AL-2.5V fasteners also?

A: Yes we have the material bar of Titanium Ti-3AL-2.5V, and can produce this titanium bolts/screws, and other machined parts, we can manufacture according to customers' design either, welcome to contact us.

Q: Does your Ti-3AI-2.5V alloy rod and bar support OEM customization?

A: Yes we accept OEM customization, can make according to customers' requests.

Q: What is the delivery time on the titanium Ti-3AI-2.5V alloy rod and bar ?

A: Normally we have the stocks for the ordinary sizes and for special size the delivery time will be within 15days.

 

About our factory

 

Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel,Zirconium products. With high quality controlling system, our products meeting the international standard as ASTM, ASME, AMS, JIS, DIN, TOCT, our main products including bars/rods, plates/sheets, tubes, wires, forgings rings, anodes, fasteners and CNC machined parts.

 

For over 11 years,Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.

product-553-352

*TO BE YOUR RELIABLE AND TRUSTABLE PARTNER AS ALWAYS!!*

 

More Detail Picture Showcase of Ti-3AI-2.5V alloy rod and bar

 

image005
image007
image009
image011

 

About Shipping

 

** By express: DHL, UPS, FEDEX, TNT, SF, Postal express.(around 4~5 days)

** By air cargo (around 5~7 days)

** By sea/ocean (around 12~25 days)

 

image013

Hot Tags: ti-3ai-2.5v alloy rod and bar, China ti-3ai-2.5v alloy rod and bar manufacturers, suppliers, factory, titanium cost, 3mm titanium rod, titanium bar price, titanium round bar for sale, 1 inch titanium round stock, titanium bar price per kg

Send Inquiry

(0/10)

clearall