Introduction of Titanium rod medical
Titanium rod medical are specialized titanium and titanium alloy rods designed for medical implants and surgical instruments. Their core advantages are excellent biocompatibility, mechanical properties that match human tissue, and corrosion resistance and non-toxicity. They are currently the core base material for implantable devices in fields such as orthopedics, dentistry, and neurosurgery.
Titanium rod medical are rod-shaped products made from titanium alloy as the base material. They possess characteristics such as low density, high strength, strong corrosion resistance, and excellent biocompatibility, and are widely used in medical fields such as orthopedic implants and surgical instruments. The material must comply with international standards such as ASTM-F136, and can withstand extreme temperature environments ranging from -273°C to 500°C without causing rejection reactions.
Main grades and key parameters of Titanium rod medical
Titanium rod medical are divided into pure titanium and titanium alloy types, both of which have clear medical standards (ASTM F67, ASTM F136, and international ISO 5832). The grades correspond to specific performance characteristics and cannot be used interchangeably.
1. Medical Grade Pure Titanium Rods (GR1ELI, GR2ELI, GR3ELI)
Core Identifier: ELI = Extra Low Interstitial, ultra-low interstitial elements, strict control of O, N, and H content to avoid brittleness and improve biocompatibility.
Key Chemical Composition (National Standard GB/T 13810, core control of interstitial elements)
| Grade | Ti (≥) | O (≤) | N (≤) | H (≤) | Fe (≤) | C (≤) | Core Characteristics
| GR1ELI | 99.85 | 0.12 | 0.03 | 0.012 | 0.20 | 0.05 | Best plasticity, lowest strength, soft state
| GR2ELI | 99.75 | 0.16 | 0.05 | 0.012 | 0.30 | 0.05 | Moderate strength, excellent plasticity, most commonly used
| GR3ELI | 99.50 | 0.20 | 0.05 | 0.012 | 0.30 | 0.05 | Highest strength, slightly reduced plasticity, suitable for load-bearing applications
Mechanical Properties (Annealed state, standard state for medical titanium rods)
Tensile strength ≥ 345-500MPa, Yield strength ≥ 240-380MPa, Elongation ≥ 18%-25%, Hardness HV120-180, Non-magnetic
Suitable applications: Dental implants, bone screws, soft tissue fixation devices, GR2ELI is the preferred choice (highest cost-effectiveness)
2. Medical Grade Titanium Alloy Rod (Ti-6Al-4V ELI, the only mainstream medical titanium alloy)
Core Composition: Ti-6Al-4V ELI, ultra-low interstitial elements, Al and V content are strictly controlled (to prevent ion leaching), making it the preferred medical titanium alloy (no other medical titanium alloy is used on a large scale).
Key Chemical Composition:
Ti balance, Al 5.5-6.5%, V 3.5-4.5%, O≤0.13%, N≤0.05%, H≤0.012%, Fe≤0.25%, C≤0.05%
Mechanical Properties (Annealed state, ideally suited for load-bearing applications):
Tensile strength ≥860MPa, Yield strength ≥795MPa, Elongation ≥10%, Hardness HV280-350, Elastic modulus 110GPa, Excellent fracture toughness
Key Features: Strength is significantly higher than medical grade pure titanium, mechanically matches human load-bearing bones (such as the femur and tibia), good fatigue resistance, and less prone to fracture during long-term implantation.
Suitable Applications: Orthopedic joint replacement, spinal fixation rods, femoral prostheses, load-bearing bone screws; it is the core base material for orthopedic implants.
Typical application scenarios for Titanium rod medical
Medical titanium rods must be selected according to the implantation site and load-bearing requirements, and are not interchangeable. Specific applications are as follows:
Orthopedics (largest usage):
Load-bearing areas: Femur, tibia, spine → TI6AL4V ELI titanium rods (φ5-30mm), used for making joint prostheses, spinal fixation rods, and intramedullary nails, utilizing their high strength and fatigue resistance.
Non-load-bearing areas: Phalanges, metacarpals, ribs → GR2 ELI titanium rods (φ3-10mm), used for making bone screws and bone plates, utilizing their high plasticity and ease of shaping.
Dentistry:
Dental implants: GR2 ELI titanium rods (φ3-6mm), precision machined + surface sandblasting/acid etching to enhance osseointegration, suitable for alveolar bone implantation.
Orthodontic brackets, archwires: GR1 ELI titanium rods (φ1-3mm), good plasticity, can be bent and shaped, non-allergenic.
Neurosurgery: Cranial fixation, minimally invasive spinal fixation → GR2 ELI/TI6AL4V ELI titanium rods (φ2-8mm), moderate strength, non-magnetic, does not affect magnetic resonance imaging (MRI) examinations.
Other fields: Cardiovascular stents (thin diameter GR1ELI titanium rods φ0.5-2mm), cochlear implants (GR2 ELI titanium rods), utilizing their resistance to body fluid corrosion and biocompatibility advantages.
Core principles for selecting Titanium rod medical
- Non-load-bearing / requiring bending and shaping: Choose GR1ELI or GR2ELI (GR2ELI is preferred for its best cost-effectiveness).
- Light load-bearing / requiring a balance of strength: Choose GR3ELI.
- Load-bearing / requiring fatigue resistance: TI6AL4V ELI is a must (no substitute).
- High-end, vanadium-free applications: Choose the niche Ti-6AL-7Nb ELI.
Products Picture show of Titanium rod medical






About our company

TO BE YOUR RELIABLE AND TRUSTABLE PARTNER AS ALWAYS!
We Baoji Reliab Metal Material Co.,Ltd was founded in year 2013, located in the famous 'China Titanium Valley--BAOJI', under the strong R&D ability and continuously development, our mainly products have including titanium&titanium alloy bars/rods, plates, tubes, forgings, fasteners&machined parts, and nickel products. We have passed the Quality System Certificate of ISO 9001-2015, aiming for the satisfactions of different customers' requests.
how to contact us
E-mail: garychen3215@hotmail.com
Address: No.35, Baoti Rd, Baoji city, Shaanxi Province, China
Contact: Mr. Gary Chen
Phone: +86-917-8883215
Mobile/WhatsApp: +86 13092900605
Hot Tags: titanium rod medical, China titanium rod medical manufacturers, suppliers, factory, titanium necklaces, 1 titanium bar, 6mm titanium rod, titanium rectangular bar, 3mm titanium rod, titanium welding electrode