Introduction of Titanium Timascus plate
What is the Titanium Timascus plate?
Titanium Timascus Plates/Sheets (or named Mokuti) is composed of two or three Grades titanium alloy(typically pure titanium alloy and Ti6Al4V), Titanium damascus is made by forged welding with heat and pressure to have different grade titanium alloy to forge laminated together .
The different titanium alloys color through the use of heat or anodizing. Each sort of titanium alloy has the potential for a new color.
Because only the general direction and number of layers of the pattern can be controlled during the processing, so that each Timascus plate is unique.
Brief Data of Titanium Timascus plate
Standard: ASTM B265, ASTM F67,AMS 4911
Grade:Gr.1 Gr.2 Gr.3 Gr.5 Gr.7 Gr.9 Gr.12
Manufacturing Processes:Rolling, Forging, Annealing
Size:Thickness0.8mm~50.0mm*Width100mm~1500mm*Length1000mm~6000mm
Features: The excellent properties of Titanium Plates include high strength, low density, good mechanical properties, corrosion resistance, high stability and so on. So Titanium & Titanium Alloy Plates always be used in airplane engine components, rockets, missile and other aircraft components.
In addition to that, titanium and titanium alloy plates also can be used in industrial construction , sports equipment, tableware, outdoor supplies and so on. The good performances of titanium plates make it easy to be accept and are more and more familiar by public.
Rolling Processing of Titanium Timascus Plates/Sheets
(1)Hot Rolled Processing:
Hot rolling is carried out above the recrystallization temperature of titanium alloys and is suitable for the production of medium-thickness plates (such as those with a thickness of more than 5mm). Hot rolling can enable titanium alloy plates to obtain good internal structure and mechanical properties, and improve the plasticity and toughness of the plates.
(2)Cold Rolled Processing:
Cold rolling is a rolling process carried out at room temperature, and is mainly used for the production of thin plates (such as those with a thickness ranging from 0.3 to 5mm), which can achieve higher surface accuracy and dimensional accuracy. The surface of the cold-rolled titanium alloy sheet is smooth and the thickness is uniform, making it suitable for components with high requirements for the surface quality of the sheet.
(3)Comparison of Rolling Processes:
Hot rolling and cold rolling both have their own advantages and disadvantages.
Hot rolling has a high production efficiency, but its surface quality is relatively poor.
Cold-rolled surfaces have good quality, but the production cost is relatively high.
In actual production, the appropriate rolling process can be selected according to the product requirements.
Picture Showcase of Titanium Timascus Plate




About Our Factory
Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel,Zirconium products. With high quality controlling system, our products meeting the international standard as ASTM, ASME, AMS, JIS, DIN, TOCT, our main products including bars/rods, plates/sheets, tubes, wires, forgings rings, anodes, fasteners and CNC machined parts.
For over 11 years,Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.

*TO BE YOUR RELIABLE AND TRUSTABLE PARTNER AS ALWAYS!!*
FAQ
Q: Can you make special size of the Titanium Timascus Plate?
A: Yes we can any size according to customer's requests
Q: What are the advantages of the titanium Timascus Plate ?
A: Titanium Timascus Plate is light in specific gravity, and has high strength, pattern unique, can make and show beautiful colors(with several layers), can be used to make EDC parts.
Q: How does the titanium timascus plates been shipped?
A: We can ship out the goods by international express(like DHL, UPS, FedEx), Air cargo, and Ocean/sea shipping.
Q: Where is your company located in?
A: We are in Baoji city, Shaanxi province, Northwest of China.
Q: How to contact your company?
A: Our e-mail address is garychen3215@hotmail.com, WhatsApp account is 0086 13092900605, WeChat number is 86 13092900605, welcome to contact us for any inquiry.
Hot Tags: titanium timascus plate, China titanium timascus plate manufacturers, suppliers, factory, titanium gold price, titanium magnetic, titanium flat stock, titanium wrought alloy plate, titanium steel, titanium tubing